ASTM A240 316L plak asye pur
1. estanda: ASTM A240, ASME SA240
2. pesè: 0.3mm - 50 milimèt
3. Lajè: 600 a 2500mm oswa Customized
4. Longè: 1000mm-6000mm oswa Customized
5. Klas: SUS 316l, UNS S31600, EN 1.4301
ASTM A240 316L plak asye pur, se yon alyaj asye ki gen omwen 10.5% oswa 11% CHROMIUM. 316L se yon vèsyon ki ba kabòn nan 316 epi li pa afekte pa sansibilizasyon (presipitasyon nan karbid nan limit grenn). Se poutèt sa, li se lajman ki itilize pou gwo konpozan soude (apeprè 6 mm ak pi wo a). ASTM A240 Kalite 316L Plak se ki pa mayetik nan kondisyon an rkwit. Plak 316L gen bon rezistans korozyon frèt nan anviwònman kriyojenik. Li se ideyal pou divès endistri tankou pwosesis chimik ak aplikasyon pou maren.
Aplikasyon pou plak 316L SS yo enkli:
- Endistri twal ak papye, osi byen ke tretman dlo ak sistèm raffinage lwil oliv.
- Veso presyon, tank, bride, echanjeur chalè, sistèm kanalizasyon, tiyo ekipman ak ponp.
- Pwosesis chimik ak depo.
- Bilding bò lanmè, balistrad bò lanmè ak ekipman maren.
- Plak TP316L kapab tou fèt nan tiyo, ekipman, nwa, boulon, vis, bride ak sous dlo.

ASTM A240 Kalite 316L Nerjaveèi Plak Espesifikasyon
| Spesifikasyon | ASTM A240 / ASME SA240 |
| Faktori | Woule cho (HR) / woule frèt (CR) |
| Epesè | 0.3 MM pou 50 MM Epesè |
| Lajè | 1250 MM / 1500 MM / 2000 MM / 04 Pye / 05 Pye ak Lajè Koupe Custom dapre egzijans |
| Longè | 2400 MM / 2420 MM / 6000 MM / 08 Pye / 10 Pye / Koupe Bobin ak Longè Koupe Custom dapre egzijans |
| Sifas fini | 2B, 2D, BA, MATT, MATT PVC, No.4, No.5, SB, HR, No.8, Iwa, Hairline, Bwòs, Textured, baz lwil oliv mouye Poli, Tou de bò poli disponib. |
| Kouch | PVC kouch nòmal / lazè, fim: 100 mikromèt, koulè: nwa / blan. |
| Tès | NACE MR0175, TÈS ultrason, TÈS IGC, Tès enpak Charpy, Macro, Gwosè grenn, dite, elatriye. |
| Sèvis te ajoute | Koupe gaz / CNC Plasma Koupe / Tòl Fabrication / Profilage / Woule / Koube / Egzèsis / Punch / Machining / sab eksplozif / Tretman chalè |
| Sètifika tès | Sètifika Tès Manifakti Dapre EN10204 3.1, 3.2 / Anba Ajans Enspeksyon Twazyèm Pati Tankou SGS, ABS, TUV, DNV, LLOYDS |
ASTM A240 Nerjaveèi asye 316L konpozisyon chimik
| Klas | C | Ni | Si | N | S | Mn | P | Kr | Mo | |
| SS 316L | min. | – | 10.0 | – | – | – | – | – | 16.0 | 2.00 |
| max. | 18.0 | 14.0 | 0.75 | 0.10 | 0.03 | 2.00 | 0.045 | 18.0 | 3.00 | |
ASME SA240 SS 316L Plak Pwopriyete mekanik
| Klas | Fòs rupture (MPa) min | Elongasyon (% nan 50mm) min | Sede Fòs 0.2% Prèv (MPa) min | Dite | |
| Rockwell B (HR B) max | Brinell (HB) max | ||||
| 316L | 485 | 40 | 170 | 95 | 217 |
Koyefisyan ekspansyon tèmik lineyè
| Ranje Tanperati | Koefisyan | ||
| degre F | degre | nan/nan/ degre F | cm / cm / degre |
| 68 - 212 | 20 - 100 | 9.2 x 10-6 | 16.5 x 10-6 |
| 68 - 932 | 20 - 500 | 10.1 x 10-6 | 18.2 x 10-6 |
| 68 - 1832 | 20 - 1000 | 10.8 x 10-6 | 19.5 x 10-6 |
Espesifik Chalè ASTM A240 TP 316L Nerjaveèi Plak
| degre F | degre | Btu/lb• degre F | Jkg•K |
| 68 | 20 | 0.108 | 450 |
| 200 | 93 | 0.116 | 485 |
Konduktivite tèmik nan ASTM A240 SS 316L Plak
| degre F | degre | Btu•nan/hr•ft2• degre F | W/m•K |
| 68 - 212 | 20 - 100 | 100.8 | 14.6 |
ASTM A240 316L Tolerans plak asye pur
| ASTM A240 316L Plak | Lajè (w), pous [mm] | |||
| Espesifye epesè (t), pous [mm] | w Mwens pase oswa egal a 84 [2134] | 84 [2134] < w Mwens pase oswa egal a 120 [3048] | 120 [3048] < w Mwens pase oswa egal a 144 [3658] | w > 144 [ 3658] |
| Tolerans sou epesè espesifye, pous [mm] | ||||
| t < 3/16 [4.76] | 0.055 [1.35] | 0.070 [1.78] | - | - |
| 3/16 [4.76] Mwens pase oswa egal a t < 3/8 [9.52] | 0.045 [1.14] | 0.050 [1.27] | 0.085 [2.16] | - |
| 3/8 [9.52] Mwens oswa egal a t < 3/4 [19.05] | 0.055 [1.40] | 0.060 [1.52] | 0.085 [2.16] | 0.090 [2.29] |
| 3/4 [19.05] Mwens pase oswa egal a t < 1 [25.04] | 0.060 [1.52] | 0.065 [1.65] | 0.085 [2.16] | 0.100 [2.54] |
| 1 [25.40] Mwens pase oswa egal a t < 2 [50.80] | 0.070 [1.78] | 0.075 [1.90] | 0.095[2.41] | 0.115 [2.92] |
| 2 [ 50.80] Mwens pase oswa egal a t < 3 [76.20] | 0.125 [3.20] | 0.150[3.80] | 0.175 [4.45] | 0.200 [5.08] |
| 3 [76.20] Mwens pase oswa egal a t < 4 [101.6] | 0.150 [3.81] | 0.160 [4.06] | 0.200 [5.08] | 0.225 [5.72] |
| 4 [101.6] Mwens pase oswa egal a t < 6 [152.4] | 0.180 [4.75] | 0.200 [5.08] | 0.335 [8.50] | 0.355 [9.02] |
| 6 [152.4] Mwens pase oswa egal a t < 8 [203.2] | 0.235 [6.00] | 0.255 [6.48] | 0.355 [9.02] | 0.435 [11.0] |
| 8 [203.2] Mwens oswa egal a t < 10 [254.0] | 0.315 [8.00] | 0.335 [8.50] | 0.435 [11.0] | 0.550 [14.0] |
Tretman Chalè nan TP316L Plak Fèy Strip
Austenitic Nerjaveèi yo apwovizyone nan kondisyon an rkwit faktori. Pou 316 L alyaj, solisyon annealing fèt pa chofaj nan ranje tanperati a nan 1900 a 2150 degre F (1040 a 1175 degre) ki te swiv pa lè refwadisman oswa dlo asouvisman depann sou epesè nan seksyon. Rapid refwadisman nan seri 1500 a 800 degre F (816 a 427 degre) pou fè pou evite re-presipitasyon nan karbid chromium bay pi bon rezistans korozyon.
TP316L Plak Fèy Band Kalite Anbalaj:
- Pakèt (egzagonal)
- Bwat an bwa
- Kès (asye/bwa)
- Kès espesyal pou U-bends, separe pou chak reyon
- Chak pake kouvri ak plastik pou pwoteje li kont move tan
- Plak asye pur alyaj 316L yo pwoteje pa bann plastik
- Pakèt mare ak espageti plastik.
- Yon lis anbalaj (laminated) vini ak kès la
FAQ
K: Konsènan ASTM A240 316L pri plak asye pur pou chak kg?
K: Konbyen tan tan livrezon ou pran?
K: Èske gen sèvis echantiyon?
K: Ki kantite minimòm lòd?
K: Ki jan yo pake pwodwi yo?
K: Peyi ekspòte yo
Baj popilè: astm a240 316l plak asye pur, plak asye pur 316l, plak 316l
Ou ka renmen tou
Voye rechèch