ASTM A240 Nerjaveèi asye Plak Fèy
1. estanda: ASTM A240 / ASME SA240
2. epesè: 0.1mm-200 milimèt
3. Lajè: 1000-3000mm
4. Longè: 1000-6000mm
ASTM A240 plak asye purs genyen ladan yo 317L, 321, 347, 2205, 2507, 254smo, 904l ak lòt alliages. ASTM A240 kouvri chromium, chromium-nikèl ak chromium-manganèz-nikèl plak asye pur, fèy papye ak bann pou veso presyon ak itilizasyon jeneral. Plak asye pur yo reziste korozyon epi yo ka itilize pou yon tan long nan anviwònman imid ak korozivite.Plak asye purtou gen karakteristik sa yo nan fòs segondè, rezistans chalè, pwosesis fasil ak bon aparans. Konpayi nou an se yon founisè plak asye pur ak eksperyans ekspòtasyon 15+. Kontakte nou pou plis enfòmasyon ak quotes gratis!
SA240 Nerjaveèi asye Plak FèyEstanda:
- ASTM A240: Spesifikasyon pou Kwòm ak Chromium-Nikèl Nerjaveèi plak, fèy, ak teren pou veso presyon ak pou aplikasyon jeneral
- Lòt pwodwi: Nou se youn nan manifaktirè yo enpòtan, founisè, ak ekspòtatè nan ekipman, bride, Fastener, ekipman tiyo, tiyo, tib, plak / fèy / bann / bobin, ba / baton, elatriye nan divès kalite materyèl.

ASTM A240 Nerjaveèi asye plak fèy espesifikasyon retire rad sou ou
| Espesifikasyon | ASTM A240 / ASME SA 240 |
| Epesè | Woule frèt:0.15mm-10mm |
| Woule cho: 3.0mm-180mm | |
| Fini | 2B, 2D, 4B, BA, HL, IWA, bwòs, NON. 1-NON. 4, 8K, ak sou sa |
| Lajè | {{0}mm |
| Longè | 1000mm-11000mm oswa kòm kondisyon kliyan an |
| Estanda | ASME, ASTM, EN, BS, GB, DIN, JIS, elatriye |
| Materyèl | Sitou: 304, 304L, 304H, 316, 316L, 316Ti, 2205, 321, 310S, 347H |
| 300series: 310, 310S, 316, 316L, 316Ti, 317L, 321, 347 | |
| Duplex Nerjaveèi: S31803, S32205, S32750, S32760 | |
| Espesyal Nerjaveèi: 904L, 347/347H, 317/317L, 316Ti, 254SMO | |
| Pake | kondisyon kliyan yo ak estanda ekspòtasyon lanmè-merite procesna |
| Tan livrezon | 7-45 jou dapre egzijans kliyan an ak kantite |
ASTM A240 SS Plak Chimik Konpozisyon
| Klas | C Mwens pase oswa egal a | Mn | P Mwens pase oswa egal a | S Mwens pase oswa egal a | Si mwens pase oswa egal a | Kr | Mouvman | Ni | Taks | N |
| 304 | 0.07 | 2 | 0.045 | 0.03 | 0.75 | 17.5-19.5 | - | 8.0-10.5 | - | - |
| 304L | 0.03 | 2 | 0.045 | 0.03 | 0.75 | 17.5-19.5 | - | 8.0-12.0 | - | - |
| 304H | 0.04-0.10 | 2 | 0.045 | 0.03 | 0.75 | 18.0-20.0 | 8.0-10.5 | - | - | |
| 316 | 0.08 | 2 | 0.045 | 0.03 | 0.75 | 16.0-18.0 | 2.00-3.00 | 10.0-14.0 | - | - |
| 316L | 0.035 | 2 | 0.045 | 0.03 | 0.75 | 16.0-18.0 | 2.00-3.00 | 10.0-14.0 | - | - |
| 316Ti | 0.08 | 2 | 0.045 | 0.03 | 0.75 | 16.0-18.0 | 2.00-3.00 | 10.0-14.0 | - | - |
| 317 | 0.08 | 2 | 0.045 | 0.03 | 0.75 | 18.0-20.0 | 3.0-4.0 | 11.0-15.0 | - | - |
| 317L | 0.03 | 2 | 0.045 | 0.03 | 0.75 | 18.0-20.0 | 3.0-4.0 | 11.0-15.0 | - | - |
| 321 | 0.08 | 2 | 0.045 | 0.03 | 0.75 | 17.0-19.0 | - | 9.0-12.0 | - | - |
| 310S | 0.08 | 2 | 0.045 | 0.03 | 1.5 | 24.0-26.0 | - | 19.0-22.0 | - | - |
| 347 | 0.08 | 2 | 0.045 | 0.03 | 0.75 | 17.0-19.0 | - | 9.0-13.0 | - | - |
| 254SMO | 0.02 | 1 | 0.03 | 0.01 | 0.8 | 19.5-20.5 | 6.0-6.5 | 17.5-18.5 | 0.5-1.0 | - |
| AL-6XN | 0.03 | 2 | 0.04 | 0.03 | 1 | 20.0-22.0 | 6.0-7.0 | 23.5-25.5 | 0.75 | - |
| F904L | 0.02 | 2 | 0.045 | 0.035 | 1 | 19.0-23.0 | 4.0-5.0 | 23.0-28.0 | 1.0-2.0 | - |
| S31803 | 0.03 | 2.00 | 0.03 | 0.02 | 1.00 | 21.0–23.0 | 2.5–3.5 | 4.5–6.5 | - | 0.08–0.20 |
| S32205 | 0.03 | 2.00 | 0.03 | 0.02 | 1.00 | 22.0–23.0 | 3.0–3.5 | 4.5–6.5 | - | 0.14–0.20 |
| S32750 | 0.03 | 1.20 | 0.035 | 0.02 | 0.80 | 24.0-26.0 | 3.0-5.0 | 6.0-8.0 | 0.5 | 0.24-0.32 |
| S32760 | 0.03 | 1.00 | 0.03 | 0.01 | 1.00 | 24.0-26.0 | 3.0-4.0 | 6.0-8.0 | 0.50–1.00 | 0.20-0.30 |
Pwopriyete mekanik ASTM A240 Fèy asye pur
| Pwopriyete mekanik | Tensile, min, ksi[MPa] | Sede, min, ksi[MPa] | Elongasyon, % (min) |
| 304 | 75【515】 | 30【205】 | 40 |
| 304L | 70【485】 | 25【170】 | 40 |
| 304H | 75【515】 | 30【205】 | 40 |
| 316 | 75【515】 | 30【205】 | 40 |
| 316L | 70【485】 | 25【170】 | 40 |
| 316Ti | 75【515】 | 30【205】 | 40 |
| 317 | 75【515】 | 30【205】 | 35 |
| 317L | 75【515】 | 30【205】 | 40 |
| 321/H | 75【515】 | 30【205】 | 40 |
| 310S | 75【515】 | 30【205】 | 40 |
| 347/H | 75【515】 | 30【205】 | 40 |
| S31254 | 95【655】 | 44【305】 | 35 |
| N08367 | 95【655】 | 45【310】 | 30 |
| N08904 | 71【490】 | 31【220】 | 35 |
| S31803 | 90【620】 | 65【450】 | 25 |
| S32205 | 95【655】 | 65【450】 | 25 |
| S32750 | 116【800】 | 80【550】 | 15 |
| S32760 | 108【750】 | 80【550】 | 25 |
ASTM A240 Nerjaveèi asye plak fèy ak klasifikasyon teren
- Plak asye pur: Plak yo se pwodwi woule plat ki gen yon epesè ki gen plis pase 3/16 pous [5 mm] ak yon lajè ki gen plis pase 24 pous [600 mm].
- Fèy Nerjaveèi: Plak yo se pwodwi woule plat ki gen yon epesè mwens pase 3/16 pous [5 mm] ak yon lajè ki gen plis pase 24 pous [600 mm].
- Bann asye pur: Strip se yon pwodwi plat trè mens, pandan y ap teren se yon pwodwi plat woule frèt ak yon epesè mwens pase 3/16 "[5 mm] ak yon lajè mwens pase 24" [600 mm].
SS ASTM A240 Plak, Fèy, Faktori teren
Materyèl yo anvan tout koreksyon (anjeneral dal oswa lengote) pou pwodwi asye pur plat woule yo ta dwe pwodwi pa ark oswa endiksyon k ap fonn oswa refonn, dal cho-woule, chalè-trete rkwit, ak eksplozyon-netwaye oswa marinated, ak bon jan kalite teste.
Estanda referans fèy plak asye pur
- ASTM A 370 Metòd ak definisyon pou tès mekanik nan pwodwi asye
- ASTM A 480/A 480M Standard Spesifikasyon pou plat Nerjaveèi asye ak chalè reziste plak, fèy, ak teren
- ASTM A 923 Metòd tès pou enklizyon metal prejidis nan duplex Austenitic / Feritic Nerjaveèi Forgings
- ASTM E 112 Metòd pou Detèminasyon Gwosè Mwayèn Grenn Metal yo
- ASTM E 527 Metal Alloys (UNS) Metòd nimero
- SAE J 1086 Metal Alloys (UNB) Metòd nimero
FAQ
K: Konsènan ASTM A240 pri plak asye pur?
K: Konbyen tan tan livrezon ou pran?
K: Èske gen sèvis echantiyon?
K: Ki kantite minimòm lòd?
K: Ki jan yo pake pwodwi yo?
K: Peyi ekspòte yo
Baj popilè: astm a240 plak asye pur, plak asye pur, plak astm a240, fèy asye pur