S31803 Duplex fèy asye pur
1. estanda: ASTM A240 / ASME SA240
2. Epesè: 0.5mm-30mm
3. Lajè: 1000-2500mm
4. Longè: 1000-6000mm
5. Ekivalan:UNS S31803, WNR.1.4462
S31803 Duplex fèy asye purkonpozisyon gen ladan 20% chromium, 3% molybdène, 6% nikèl, 0.2% nitwojèn, elatriye. Yon mikwostrikti de-faz ki gen ladan faz ferit ak ostenit. Li gen bon rezistans nan korozyon estrès sulfid ak gwo rezistans nan krak korozyon estrès klori, tankou dlo lanmè, medya asid ak alkalin, elatriye. de fwa fòs sede austenitic Nerjaveèi 316L ak 317L. Konpayi nou an se yon founisè 2205 ak 15+ eksperyans ekspòtasyon,kontakte noupou plis enfòmasyon ak quotes gratis!
ASTM A240S31803 duplex plak asye purestanda:
- ASTM A240: Spesifikasyon pou Kwòm ak Chromium-Nikèl Nerjaveèi plak, fèy, ak teren pou veso presyon ak pou aplikasyon jeneral
- Lòt Klas: 304, 304L, 316, 316L, 316Ti, 310S, 317, 317L, 321, 347, 904L, S31254, N08367, UNS S32205, UNS S31803, UNS S31803, Et.

S31803 Duplex Nerjaveèi Fèy Espesifikasyon
| Espesifikasyon | ASTM A240 / ASME SA240 |
| Epesè |
0.5mm-30mm |
| Lajè | 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, elatriye |
| Longè | 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, elatriye |
| Sifas | 2B, 2D, BA, NO.1, NO.4, NO.8, 8K, glas, karo, Relief, cheve, eksplozyon sab, bwòs, grave, elatriye |
| Fini | Plak woule cho (HR), fèy woule frèt (CR), 2B, 2D, BA NO (8), SATIN (Met ak plastik kouvwi) |
| Fòm | Bobin, Feuilles, Woulo, Plain Sheets, Shim Sheets, Perforation Sheets, Checkered Plates, Strips, Flats, Blank (Sèk), Bag (Flange), elatriye. |
Pwa ASME SA 240 UNS S31803 Fèy
| Epesè | Pwa plak pou chak zòn inite | Dansite |
|---|---|---|
| 3/16 pous | 0.06000 lbs/pous²42.184176 kg/m² | 0.315 lbs/in³8.72 g/cm³ |
| 1/4 pous | 0.08 lbs/pous²56.245568 kg/m² | 0.315 lbs/in³8.72 g/cm³ |
| 3/8 pous | 0.121 lbs/pous²85.0714216 kg/m² | 0.315 lbs/in³8.72 g/cm³ |
| 1/2 pous | 0.161 lbs/pous²113.1942056 kg/m² | 0.315 lbs/in³8.72 g/cm³ |
| 5/8 pous | 0.196 lbs/pous²137.8016416 kg/m² | 0.315 lbs/in³8.72 g/cm³ |
| 3/4 pous | 0.235 lbs/pous²165.221356 kg/m² | 0.315 lbs/in³8.72 g/cm³ |
| 7/8 pous | 0.274 lbs/pous²192.6410704 kg/m² | 0.315 lbs/in³8.72 g/cm³ |
| 1 pous | 0.313 lbs/pous²220.0607848 kg/m² | 0.315 lbs/in³8.72 g/cm³ |
| 1 1/4 pous | 0.391 lbs/pous²274.9002136 kg/m² | 0.315 lbs/in³8.72 g/cm³ |
| 1 1/2 pous | 0.47 lbs/pous²330.442712 kg/m² | 0.315 lbs/in³8.72 g/cm³ |
| 1 3/4 pous | 0.549 lbs/pous²385.9852104 kg/m² | 0.315 lbs/in³8.72 g/cm³ |
| 2 pous | 0.627 lbs/pous²440.8246392 kg/m² | 0.315 lbs/in³8.72 g/cm³ |
UNS S31803 Pwopriyete mekanik
- Fòs sede: Pi gran pase oswa egal a 450 MPa
- Fòs rupture: Pi gran pase oswa egal a 620 MPa
- Elongasyon: pi gran pase oswa egal a 25%
- Enpak severite: Satisfè kondisyon yo
ASME SA240 UNS S31803 Steel Sheet Application
- Endistri lwil oliv ak gaz natirèl
- Endistri chimik
- Echanjeur chalè
- Oseyan jeni
- Endistri pwosesis manje
FAQ
K: Konsènan S31803 Duplex Nerjaveèi asye pri fèy pou chak kg?
K: Konbyen tan tan livrezon ou pran?
K: Èske gen sèvis echantiyon?
K: Ki kantite minimòm lòd?
K: Ki jan yo pake pwodwi yo?
K: Peyi ekspòte yo
Baj popilè: duplex ss s31803, duplex fèy asye pur, duplex fèy asye, s31803 duplex
Ou ka renmen tou
Voye rechèch