ASTM A312 317 Tiyo Nerjaveèi
1. estanda: ASTM A312 / ASME SA312
2. Gwosè: 1/8"- 30"
3. pesè: SCH5 ~ SCHXXS
4. ekivalan: UNS S31700, WNR.1.4449, AISI 317
ASTM A312 317 Tiyo Nerjaveèise yon molybdène ki gen austenitic Nerjaveèi ak amelyore rezistans korozyon, segondè fòs rupture ak ekselan rezistans chalè.WNR.1.4449Anplis de molybdène amelyore rezistans korozyon nan yon varyete de pwodwi chimik, ki gen ladan asid silfirik, asid acetic ak lòt asid òganik. Nou se yonSS 317 tiyofounisè ki gen 15+ eksperyans ekspòtasyon, kontakte nou pou plis enfòmasyon ak sitasyon gratis!
ASTM A312 317 SS tiyo estanda:
- ASTM A312: Espesifikasyon estanda pou tiyo asye pur san pwoblèm, soude, ak lou travay frèt.
- Klas: TP304, TP304L, TP310S, TP316, TP316L, 316Ti, TP317, TP317L, TP321, TP347, TP347H, S31254, N08367, N08926, N081904, N03
- ANSI B36.19: Spesifikasyon pou tiyo asye pur

ASTM A312 TP317 Espesifikasyon tiyo asye pur
| Espesifikasyon | ASTM A 312 / ASME SA 312 |
| Dimansyon | ASTM, ASME, ak API |
| SS 317 Tiyo | 1/2″ NB – 16″ NB |
| ERW 317 Tiyo | 1/2″ NB – 24″ NB |
| EFW 317 Tiyo | 6″ NB - 100″ NB |
| Gwosè | 1/8″NB POU 30″NB NAN |
| Orè | SCH5, SCH10, SCH20, SCH30, SCH40, STD, SCH60, SCH80, XS, SCH100, SCH120, SCH140, SCH160, XXS |
| Longè | Single Random, Double Random & Koupe Longè. |
| Fen |
Plain Fen, Bizote Fen, Treaded |
| Kalite | San pwoblèm / ERW / soude / fabrike / LSAW Tiyo |
| Referans ASTM Standards |
|
Alloy 317 Nerjaveèi asye tiyo konpozisyon chimik
| Klas | C | Ni | Si | S | Mn | P | Kr | Mo | |
| SS 317 | min. | - | 11.0 | - | - | - | - | 18.0 | 3.00 |
| max. | 0.08 | 14.0 | 1.00 | 0.03 | 2.00 | 0.040 | 20.0 | 4.00 | |
ASTM A312 TP317 Pwopriyete mekanik tiyo
| Klas | Fòs rupture (MPa) min | Elongasyon (% nan 50mm) min | Sede Fòs 0.2% Prèv (MPa) min | Dite | |
| Rockwell B (HR B) max | Brinell (HB) max | ||||
| AISI 317 | 515 | 35 | 205 | 95 | 217 |
ASTM A312 317 Pwopriyete fizik tiyo asye pur
|
Pwopriyete fizik (tanperati chanm) |
||
|
Chalè Espesifik (0-100 degre) |
500 |
J.kg-1. degre K-1 |
|
Kondiktivite tèmik |
14.6 |
Wm -1. degre K-1 |
|
Ekspansyon tèmik |
16.5 |
mm / m / degre |
|
Elastisite modil |
193 |
GPa |
|
Rezistivite elektrik |
7.4 |
μohm/cm |
|
Dansite |
7.99 |
g/cm3 |
ASTM A312 TP317 Tolerans tiyo san pwoblèm
| NPS | ASTM A312 TP317 OD tolerans | |||
| + | – | |||
| pous | mm | pous | mm | |
| 1/8~1 1 /2 > 1 1 /2~4 > 4~8 > 8~18 > 18~26 > 26~34 > 34~48 |
1/64(0.015) 1/32(0.031) 1/16(0.062) 3/32(0.093) 1/8(0.125) 5/32(0.156) 3/16(0.187) |
0.4 0.8 1.6 2.4 3.2 4.0 4.8 |
1/32(0.031) 1/32(0.031) 1/32(0.031) 1/32(0.031) 1/32(0.031) 1/32(0.031) 1/32(0.031) |
0.8 0.8 0.8 0.8 0.8 0.8 0.8 |
Aplikasyon pou tiyo ASME SA312 UNS S31700
- Pwosesis chimik
- Raffinage petwòl
- Pwosesis Manje
- Endistri famasetik
- Endistri gaz natirèl
- Endistri min
Nerjaveèi asye 317 Tès Kalite tiyo
- Tès dite
- Tès ekspansyon
- Tès mikwo ak makro
- Tès Chimik
- Rapò tès PMI
- Tès Tensile
- Tès Fòs Sede
- Tès elektrik idwostatik oswa ki pa destriktif
FAQ
K: Konsènan ASTM A312 317 pri tiyo asye pur?
K: Konbyen tan tan livrezon ou pran?
K: Èske gen sèvis echantiyon?
K: Ki kantite minimòm lòd?
K: Ki jan yo pake pwodwi yo?
K: Peyi ekspòte yo
Baj popilè: 317 tiyo asye pur, a312 tiyo asye pur, 317 tiyo asye
Ou ka renmen tou
Voye rechèch