ASTM A312 tiyo asye pur
1. estanda: ASTM A312, ASME SA312
2. Kalite: san pwoblèm, soude
3. gwosè: 1/2''~48''
4. pesè: SCH5 ~ SCHXXS
Tiyo asye pur ASTM A312 se spesifikasyon estanda pou tiyo asye san pwoblèm, soude ak lou-te travay frèt austenitic. Pou itilize nan tanperati ki wo ak aplikasyon jeneral sèvis korozivite. Tiyo sa yo gen gwo fòs, ekselan rezistans korozyon, ekselan pèfòmans tanperati ki wo ak bon pwosesis.Tiyo asye pur lajman ki itilize nan lwil oliv ak gaz, pétrochimique, pwosesis manje, endistri pharmaceutique.
ASTM A312 SS tiyo estanda:
- ASTM A312: Espesifikasyon estanda pou tiyo asye san pwoblèm, soude, ak lou ki te travay frèt Austenitic Nerjaveèi.
- Estanda ASTM A312 kouvri plizyè kalite tiyo asye pur, ki gen ladan ASTM A312 tiyo san pwoblèm ak ASTM A312 tiyo soude, ak diferan klas tankou 304, 304L, 316, 316L, 321, 321H, 347, 347H, elatriye.

Konpozisyon chimik ASTM A312 Nerjaveèi tiyo
| Klas | UNS | C Mwens pase oswa egal a | Mn | P Mwens pase oswa egal a | S Mwens pase oswa egal a | Si mwens pase oswa egal a | Kr | Mo | Ni | Cu |
| TP304 | S30400 | 0.08 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | - | 8.0-11.0 | - |
| TP304L | S30403 | 0.035 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | - | 8.0-13.0 | - |
| TP316 | S31600 | 0.08 | 2 | 0.045 | 0.03 | 1 | 16.0-18.0 | 2.00-3.00 | 10.0-14.0 | - |
| TP316L | S31603 | 0.035 | 2 | 0.045 | 0.03 | 1 | 16.0-18.0 | 2.00-3.00 | 11.0-14.0 | - |
| 316Ti | S31635 | 0.08 | 2 | 0.045 | 0.03 | 0.75 | 16.0-18.0 | 2.00-3.00 | 10.0-12.0 | - |
| TP317 | S31700 | 0.08 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | 3.0-4.0 | 11.0-14.0 | - |
| TP317L | S31703 | 0.035 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | 3.0-4.0 | 11.0-15.0 | - |
| TP321 | S32100 | 0.08 | 2 | 0.045 | 0.03 | 1 | 17.0-19.0 | - | 9.0-12.0 | - |
| 321H | S32109 | 0.04-0.1 | 2 | 0.045 | 0.03 | 1 | 17.0-19.0 | - | 9.0-12.0 | - |
| 310 | S31000 | 0.25 | 2 | 0.045 | 0.03 | 1.5 | 24.0-26.0 | 0.75 | 19.0-22.0 | - |
| TP310S | S31008 | 0.08 | 2 | 0.045 | 0.03 | 1 | 24.0-26.0 | 0.75 | 19.0-22.0 | - |
| TP347 | S34700 | 0.08 | 2 | 0.045 | 0.03 | 1 | 17.0-19.0 | - | 9.0-13.0 | - |
| 254SMO | S31254 | 0.02 | 1 | 0.03 | 0.01 | 0.8 | 19.5-20.5 | 6.0-6.5 | 17.5-18.5 | 0.5-1.0 |
| AL-6XN | N08367 | 0.03 | 2 | 0.04 | 0.03 | 1 | 20.0-22.0 | 6.0-7.0 | 23.5-25.5 | 0.75 |
| F904L | N08904 | 0.02 | 2 | 0.04 | 0.03 | 1 | 19.0-23.0 | 4.0-5.0 | 23.0-28.0 | 1.0-2.0 |
ASTM A312 SS Pwopriyete mekanik tiyo
| Pwopriyete mekanik | Tensile, min, ksi[MPa】 | Sede, min, ksi[MPa】 | Elongasyon, % (min) | Dite, HB (max) |
| TP304 | 75【515】 | 30【205】 | 35 | 192 |
| TP304L | 70【485】 | 25【170】 | 35 | 192 |
| TP316 | 75【515】 | 30【205】 | 35 | 192 |
| TP316L | 70【485】 | 25【170】 | 35 | 192 |
| 316Ti | 75【515】 | 30【205】 | 35 | 192 |
| TP317 | 75【515】 | 30【205】 | 35 | 192 |
| TP317L | 75【515】 | 30【205】 | 35 | 192 |
| TP321 | 75【515】 | 30【205】 | 35 | 192 |
| 321H | 75【515】 | 30【205】 | 35 | 192 |
| TP310 | 75【515】 | 30【205】 | 35 | 192 |
| TP310S | 75【515】 | 30【205】 | 35 | 192 |
| TP347 | 75【515】 | 30【205】 | 35 | 192 |
| S31254 | 98【675】 | 43【310】 | 35 | 220 |
| N08367 | 100【690】 | 45【310】 | 30 | 241 |
| N08926 | 94【650】 | 43【295】 | 35 | 256 |
| N08904 | 71【490】 | 31【215】 | 35 | 192 |
Dimansyon nominal nan tiyo asye pur
| DN | NPS | OD (mm) dyamèt deyò |
Sch5S | Sch10S | Sch40S | Sch80S | Sch160S |
| 6 | 1/8 | 10.3 | - | 1.24 | 1.73 | 2.41 | 3.15 |
| 8 | 1/4 | 13.7 | - | 1.65 | 2.24 | 3.02 | 3.68 |
| 10 | 3/8 | 17.1 | - | 1.65 | 2.31 | 3.2 | 4.01 |
| 15 | 1/2 | 21.3 | 1.65 | 2.11 | 2.77 | 3.73 | 4.78 |
| 20 | 3/4 | 26.7 | 1.65 | 2.11 | 2.87 | 3.91 | 5.56 |
| 25 | 1 | 33.4 | 1.65 | 2.77 | 3.38 | 4.55 | 6.35 |
| 32 | 1 1/4 | 42.2 | 1.65 | 2.77 | 3.56 | 4.85 | 6.35 |
| 40 | 1 1/2 | 48.3 | 1.65 | 2.77 | 3.68 | 5.08 | 7.14 |
| 50 | 2 | 60.3 | 1.65 | 2.77 | 3.91 | 5.54 | 8.74 |
| 65 | 2 1/2 | 73 | 2.11 | 3.05 | 5.16 | 7.01 | 9.52 |
| 80 | 3 | 88.9 | 2.11 | 3.05 | 5.49 | 7.62 | 11.13 |
| 90 | 3 1/2 | 101.6 | 2.11 | 3.05 | 5.74 | 8.08 | - |
| 100 | 4 | 114.3 | 2.11 | 3.05 | 6.02 | 8.56 | 13.49 |
| 125 | 5 | 141.3 | 2.77 | 3.40 | 6.55 | 9.53 | 15.88 |
| 150 | 6 | 168.3 | 2.77 | 3.40 | 7.11 | 10.97 | 18.26 |
| 200 | 8 | 219.1 | 2.77 | 3.76 | 8.18 | 12.7 | - |
| 250 | 10 | 273.1 | 3.40 | 4.19 | 9.27 | 12.7 | - |
| 300 | 12 | 323.9 | 3.96 | 4.57 | 9.53 | 12.7 | - |
| 350 | 14 | 355.6 | 3.96 | 4.78 | 9.53 | 12.7 | - |
| 400 | 16 | 406.4 | 4.19 | 4.78 | 9.53 | 12.7 | - |
| 450 | 18 | 457 | 4.19 | 4.78 | 9.53 | 12.7 | - |
| 500 | 20 | 508 | 4.78 | 5.54 | 9.53 | 12.7 | - |
| 550 | 22 | 559 | 4.78 | 5.54 | - | - | - |
| 600 | 24 | 610 | 5.54 | 6.35 | 9.53 | 12.7 | - |
| 650 | 26 | 660 | - | - | - | - | - |
| 700 | 28 | 711 | - | - | - | - | - |
| 750 | 30 | 762 | 6.35 | 7.92 | - | - | - |
ASTM A312 Tablo tolerans dimansyon tiyo
| Estanda | Dyamèt deyò (mm) | Epesè (mm) | Longè (mm) | ||||
| ASTM A312 | 10.29~48.26 | +0.4/-0.8 | +12.5/-12.5 | +6.0/0 | |||
| 48.26~114.30 | +0.8/-0.8 | ||||||
| 114.30~219.08 | +1.6/-0.8 | ||||||
| 219.08~457.20 | +2.4/-0.8 | ||||||
Kalite pwodiksyon tiyo ASTM A312
- a. Tiyo san pwoblèm (SMLS): Tiyo san pwoblèm fèt pa pèfore yon billet solid nan asye pur.
- b. Tiyo soude (WLD): Gen ladan tiyo soude ki fabrike pa pwosesis soude otomatik (soude rezistans, soude fizyon elektrik) san yo pa ajoute metal filler pandan soude.
- c. Fwad-travay tiyo (HCW tiyo): Lou frèt-travay tiyo, ki se frèt-travay ak yon rediksyon pa mwens pase 35% nan epesè sou tou de mi yo ak soude nan tiyo a soude anvan recuit final la. Pa sèvi ak file pandan soude.
ASTM A312 SS Pipe Fabrication Services
Sèvis fabwikasyon nou yo enkli: desen ak ekspansyon, tretman chalè, travay frèt, polisaj, koube, recuit ak marinated, sablaj, machin. Founisè nou yo bay ASTM A312 tiyo san pwoblèm ak sètifika tès manifakti estanda, tès IBR, tès PMI, enspeksyon twazyèm pati SGS.
Tès ASTM A312
- Transverse oswa Longitudinal Tès Tensile
- Tès aplati
- Analiz Chimik
- Tès mekanik
- Tès ki pa destriktif
FAQ
K: Konsènan ASTM A312 pri tiyo asye pur pou chak kg?
K: Konbyen tan tan livrezon ou pran?
K: Èske gen sèvis echantiyon?
K: Ki kantite minimòm lòd?
K: Ki jan yo pake pwodwi yo?
K: Peyi ekspòte yo
Baj popilè: astm a312 tiyo asye pur, tiyo a312 ss, tiyo a312, tiyo asye pur
Ou ka renmen tou
Voye rechèch