Tib asye pur ASTM A269
1. estanda: ASTM A269, ASME SA269
2. gwosè: 1/2''~48''
3. pesè: SCH5 ~ SCHXXS
4. Kalite: San pwoblèm, soude, ERW, EFW, SAW
Tib asye pur ASTM A269se yon tib asye pur austenitic pou rezistans jeneral korozyon ak sèvis tanperati ki ba oswa segondè. Ki gen ladan ASTM A269 tib asye pur ak ASTM A269 soude tib Nerjaveèi. ASTM A269 espesifikasyon tib ki pi souvan itilize klas tiyo asye pur yoTP304, TP304L, TP304LN, TP316, TP316L, TP316LN, TP317, TP321, TP347, TP347H, S31254, N08367, N08904. Klas sa yo chwazi sou baz konpozisyon chimik yo, pwopriyete mekanik ak rezistans korozyon.
ASTM SA269 Estanda Materyèl Tib Nerjaveèi:
- ASTM A269: Espesifikasyon estanda pou tiyo asye pur Austenitic san pwoblèm ak soude pou sèvis jeneral
- Klas: TP304, TP304L, TP304LN, TP316, TP316L, TP316LN, TP317L, TP321, TP347, TP347H, 254SMO, N08367, N08904.
- Aplikasyon: Tib asye pur ASTM A269 yo itilize nan chodyèr, echanjeur chalè ak kondansateur souvan.

ASTM A269 Standard Spesifikasyon
Estanda ASTM A269 espesifye kondisyon yo pou konpozisyon chimik, pwopriyete mekanik, kouch, ak make nan tiyo. Kondisyon sa yo asire fyab ak rezistans nan tib asye pur ASME SA269. Tib A269 pwodui lè l sèvi avèk diferan metòd, ki gen ladan teknik san pwoblèm ak soude. A269 tib san pwoblèm fèt pa pèfore yon billet oswa ba ak Lè sa a, trase li sou yon mandrin yo fòme fòm nan vle ak gwosè. Soude tiyo asye pur (EFW, ERW, SAW) yo fèt pa woule yon teren asye nan yon tiyo ak Lè sa a, soude bor yo ansanm lè l sèvi avèk yon pwosesis soude rezistans wo-frekans.
ASTM A269 Nerjaveèi Tib Espesifikasyon
| Espesifikasyon tiyo | ASTM A269 / ASME SA 269 |
| Estanda tiyo | DIN, JIS, ASTM, EN, GB, AISI, ASME |
| Epesè tiyo | 0.3mm - 50 mm |
| Gwosè tiyo soude | 5.0 - 1219.2 mm |
| Dyamèt ekstèn tiyo san pwoblèm | 6.00 mm OD jiska 250 mm OD, gwosè jiska 12" NB |
| Gwosè Tib soude | 6.35 mm OD Pou 152 mm OD |
| Gwosè Tib san pwoblèm | 3.35 mm OD Pou 101.6 mm OD, 15 NB pou 150 NB IN |
| Orè tiyo | SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS |
| Tiyo & Tib Kalite | San pwoblèm / ERW / EFW / soude / fabrike tiyo |
| Tiyo & Tib Fen | Plain Fen, Bizote Fen, Treaded tiyo. |
Konpozisyon chimik ASTM A269 Tib
| Klas | DEZOLE | C Mwens pase oswa egal a | Mn | P Mwens pase oswa egal a | S Mwens pase oswa egal a | Si mwens pase oswa egal a | Kr | Mouvman | Ni | Taks |
| TP304 | S30400 | 0.08 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | - | 8.0-11.0 | - |
| TP304L | S30403 | 0.035 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | - | 8.0-13.0 | - |
| TP316 | S31600 | 0.08 | 2 | 0.045 | 0.03 | 1 | 16.0-18.0 | 2.00-3.00 | 10.0-14.0 | - |
| TP316l | S31603 | 0.035 | 2 | 0.045 | 0.03 | 1 | 16.0-18.0 | 2.00-3.00 | 11.0-14.0 | - |
| 316Ti | S31635 | 0.08 | 2 | 0.045 | 0.03 | 0.75 | 16.0-18.0 | 2.00-3.00 | 10.0-12.0 | - |
| TP317 | S31700 | 0.08 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | 3.0-4.0 | 11.0-14.0 | - |
| TP317l | S31703 | 0.035 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | 3.0-4.0 | 11.0-15.0 | - |
| TP321 | S32100 | 0.08 | 2 | 0.045 | 0.03 | 1 | 17.0-19.0 | - | 9.0-12.0 | - |
| 321H | S32109 | 0.04-0.1 | 2 | 0.045 | 0.03 | 1 | 17.0-19.0 | - | 9.0-12.0 | - |
| 310 | S31000 | 0.25 | 2 | 0.045 | 0.03 | 1.5 | 24.0-26.0 | 0.75 | 19.0-22.0 | - |
| TP310s | S31008 | 0.08 | 2 | 0.045 | 0.03 | 1 | 24.0-26.0 | 0.75 | 19.0-22.0 | - |
| TP347 | S34700 | 0.08 | 2 | 0.045 | 0.03 | 1 | 17.0-19.0 | - | 9.0-13.0 | - |
| 254 | S31254 | 0.02 | 1 | 0.03 | 0.01 | 0.8 | 19.5-20.5 | 6.0-6.5 | 17.5-18.5 | 0.5-1.0 |
| AL-6XN | N08367 | 0.03 | 2 | 0.04 | 0.03 | 1 | 20.0-22.0 | 6.0-7.0 | 23.5-25.5 | 0.75 |
| F904L | N08904 | 0.02 | 2 | 0.04 | 0.03 | 1 | 19.0-23.0 | 4.0-5.0 | 23.0-28.0 | 1.0-2.0 |
ASME SA269 Nerjaveèi tib Pwopriyete mekanik
| Pwopriyete mekanik | Tensile, min, ksi[MPa】 | Sede, min, ksi[MPa】 | Elongasyon, % (min) | Dite, HB (max) |
| TP304 | 75【515】 | 30【205】 | 35 | 192 |
| TP304L | 70【485】 | 25【170】 | 35 | 192 |
| TP316 | 75【515】 | 30【205】 | 35 | 192 |
| TP316L | 70【485】 | 25【170】 | 35 | 192 |
| 316Ti | 75【515】 | 30【205】 | 35 | 192 |
| TP317 | 75【515】 | 30【205】 | 35 | 192 |
| TP317l | 75【515】 | 30【205】 | 35 | 192 |
| TP321 | 75【515】 | 30【205】 | 35 | 192 |
| 321H | 75【515】 | 30【205】 | 35 | 192 |
| TP310 | 75【515】 | 30【205】 | 35 | 192 |
| TP310s | 75【515】 | 30【205】 | 35 | 192 |
| TP347 | 75【515】 | 30【205】 | 35 | 192 |
| S31254 | 98【675】 | 43【310】 | 35 | 220 |
| N08367 | 100【690】 | 45【310】 | 30 | 241 |
| N08926 | 94【650】 | 43【295】 | 35 | 256 |
| N08904 | 71【490】 | 31【215】 | 35 | 192 |
ASTM A269 Tib gwosè ak dimansyon
Tib asye pur ASTM A269 yo disponib nan diferan klas, gwosè ak fòm ak espesifikasyon diferan pou epesè tiyo, longè ak dyamèt. Gwosè tiyo varye ant 1/4 "a 48". Nou kapab tou Customize gwosè yo satisfè bezwen ou yo. Kontakte nou pou plis enfòmasyon ak yon quote gratis!
ASTM A269 Dimansyon Tolerans Tablo
| Dyamèt deyò (mm) | Epesè (%) | Longè (mm) | |
| D<38.1mm | +0.13mm/-0.13mm | D<12.7mm +15%/-15% D Pi gran pase oswa egal a 12.7mm +10%/-10% |
D<38.1mm +3.2/0 D Pi gran pase oswa egal a 38.1mm +4.8/0 |
| 38.1mm ~ 88.9mm | +0.25mm/-0.25mm | ||
| 88.9mm ~ 139.7mm | +0.38mm/-0.38mm | ||
| 139.7mm ~ 203.2mm | +0.76mm/-0.76mm | ||
Aplikasyon nan ASTM A269 Nerjaveèi Tib
- Endistri gaz fosil: tiyo pou transpò lwil oliv, gaz ak gaz natirèl.
- Endistri chimik: tiyo pou likid ki ba-tanperati ak wo-tanperati, gaz ak medya korozivite.
- Endistri famasetik: tiyo pou biopharmaceutique, reyaktif chimik ak dwòg.
- Endistri manje ak bwason: tiyo nan manifakti manje.
ASTM A269 TP 304 Nerjaveèi asye tib san pwoblèm anbalaj
- Pake anbalaj
- Ka an bwa
- Ka an bwa pou U Tubes
- Ranfòse pa Angle Bar
FAQ
K: Konsènan pri tib asye pur ASTM A269 pou chak kg?
K: Konbyen tan tan livrezon ou pran?
K: Èske gen sèvis echantiyon?
K: Ki kantite minimòm lòd?
K: Ki jan asire bon jan kalite pwodwi?
K: Peyi ekspòte yo
Baj popilè: astm a269 tib asye pur, tib asye pur a269, tib astm a269, tib a269