ASTM A213 TP316 Tib asye pur
1. estanda: ASTM A213 / ASME SA213
2. Gwosè: 1/8"-5"
3. pesè: 0.381 milimèt - 12.7 milimèt
4. Ekivalan: UNS S31600, WNR.1.4401, WNR.1.4436, AISI 316
ASTM A213 TP316 Tib asye purgen molybdène pou rezistans ekselan nan pitting ak kreve korozyon.S31600 fè byen nan anviwònman ki gen klori, asid silfirik, ak lòt pwodui chimik korozivite.SS 1.4401/1.4436ka itilize tanzantan nan tanperati jiska 870 degre ak kontinyèlman jiska 925 degre, epi tou li gen bon rezistans oksidasyon. Tib 316 san pwoblèm yo fèt pa pèfore billets wonn solid pou asire gwo fòs ak rezistans presyon. Nou se yonSS 316 TIBfounisè ki gen 15+ eksperyans ekspòtasyon, kontakte nou pou plis enfòmasyon ak sitasyon gratis!
ASTM A213 TP316 Tib asye pur estanda:
- ASTM A213: Espesifikasyon estanda pou chodyè asye pur feritik ak austenitik alyaj, superchofaj, ak tib echanjeur chalè
- Klas: TP310S, TP316, TP316L, 316Ti, TP317, TP317L, TP321, TP347, TP347H, S31254, N08367, N08926, N08904, S31254

Espesifikasyon Tib Nerjaveèi TP316
| SS Tib Spesifikasyon | ASTM A213, ASME SA213 |
| Estanda | GB, AISI, ASTM, DIN, EN, JIS |
| Kalite | San pwoblèm |
| OD | 1/8 "(3.18mm) OD a 5" OD (127mm) |
| Epesè | {{0}}.015"(0.38mm) - 0.5"(12.7mm) |
| Longè | Single Random, Double Random & Longè Obligatwa |
| Fen | Plain Fen, Bizote Fen, Treaded |
| Kondisyon livrezon | Rekwit ak marinated, poli, klere rkwit, frèt trase |
| Fòm | Kare / rektangilè / wonn |
| Anbalaj | Chaje nan bwat an bwa, sache plastik, bann asye fourni, oswa selon demann kliyan yo |
|
Tan livrezon |
7-45 jou |
ASME SA213 TP316 TibKONPOZISYON CHIMIK:
- Kabòn (C): Mwens pase oswa egal a 0.08%
- Silisyòm (Si): Mwens pase oswa egal a 1.00%
- Manganèz (Mn): Mwens pase oswa egal a 2.00%
- Fosfò (P): Mwens pase oswa egal a 0.045%
- Souf (S): Mwens pase oswa egal a 0.030%
- Kwòm (Cr): 16.0-18.0%
- Nikèl (Ni): 10.0-14.0%
- Molybdène (Mo): 2.0-3.0%
- Azòt (N): Mwens pase oswa egal a 0.10%
ASTM A213 TP316 TibKONPÒTMAN MECHANIK:
- Fòs Sede: Pi gwo pase oswa egal a 205 MPa
- Fòs Tensile: Pi gran pase oswa egal a 515 MPa
- Elongasyon: pi gran pase oswa egal a 35%
- Dite: 92 HRB
ASTM A213 TOLERANS DIMANSYONÈ STANDA
| Estanda | Dyamèt ekstèn (mm) | Epesè miray (mm) | Longè (mm) | |||
| Range | Devyasyon | Range | Devyasyon | Range | Devyasyon | |
| ASTM A213 | D<25.4 | 0.1/-0.1 | D Mwens pase oswa egal a 38.1 | 20%/0 | D<50.8;L mwens pase oswa egal a 7.3m | 3/0 |
| [25.4, 38.1] | 0.15/-0.15 | |||||
| (38.1, 50.8) | 0.2/-0.2 | |||||
| [50.8, 63.5) | 0.25/-0.25 | D>38.1 | 22%/0 | D Pi gran pase oswa egal a 50.8;L Mwens pase oswa egal a 7.3m | 5/0 | |
| [63.5, 76.2) | 0.3/-0.3 | |||||
| [76.2, 101.6] | 0.38/-0.38 | |||||
| (101.6, 190.5] | 0.38/-0.64 | |||||
| (190.5, 228.6] | 0.38/-1.14 | |||||
TRETMAN CHALÈ:
| Klas | UNS |
Austenitizing / Tanperati solisyon, min oswa ranje degre F [ degre ] |
Medya refwadisman |
| Nimewo | |||
| Alyaj 316 | S31600 | 1900 degre F [1040 degre] | dlo oswa lòt fre rapid |
Tiyo asye pur AISI 316APLIKASYON:
- Chimik
- Petwòl
- Petrochimik
- Famasetik
- Pwosesis Manje
- Echanjeur chalè
- Chodyèr
- Veso presyon
FAQ
K: Konsènan pri tib asye pur ASTM A213 TP316?
K: Konbyen tan tan livrezon ou pran?
K: Èske gen sèvis echantiyon?
K: Ki kantite minimòm lòd?
K: Ki jan yo pake pwodwi yo?
K: Peyi ekspòte yo
Baj popilè: 316 tib asye pur, ss 316 tib, astm a213 tp316
Ou ka renmen tou
Voye rechèch