Spesifikasyon ASTM A213 la se estanda pou tib asye pur san pwoblèm nan echanjeur chalè, chodyèr, ak surchofaj. ASTM A213 904L tib asye pur gen ekselan rezistans korozyon epi li espesyalman apwopriye pou anviwònman asid fò ak tanperati ki wo.

Estanda: ASTM A312 / ASME SA312
OD: 3.18 mm OD jiska 127 mm OD
Epesè: 0.38mm - 12.7mm
Fen: fen bizote, fen Plain
Voye rechèch
Pwodwi Entwodiksyon

ASTM A213 904L Tib asye purgen ekselan rezistans korozyon, espesyalman nan anviwònman ki gen asid silfirik ak asid fosfò. Akòz kontni an segondè nikèl, chromium ak molybdène, 904L (UNS N08904) gen ekselan rezistans nan pitting, kowozyon nan fant ak kowozyon estrès fann.SS 1.4539se anjeneral yo itilize nan tanperati ki anba a 400 degre epi li toujou kenbe rezistans korozyon li yo. EpiSS 904L tib san pwoblèmgen pi wo fòs ak rezistans konpresyon. Konpayi nou an se yonTib alyaj 904Lfounisè ki gen 15+ eksperyans ekspòtasyon, kontakte nou pou plis enfòmasyon ak sitasyon gratis!

 

ASTM A213 TP904L Estanda Tib asye pur:

  • ASTM A213: Espesifikasyon estanda pou chodyè asye pur feritik ak austenitik alyaj, superchofaj, ak tib echanjeur chalè

 

  • ASTM B677: Spesifikasyon estanda pou UNS N08904, UNS N08925, ak UNS N08926 Tiyo ak Tib san pwoblèm

 

  • Klas: TP304, TP304L, TP310S, TP316, TP316L, 316Ti, TP317, TP317L, TP321, TP347, TP347H, S31254, N08367, N08926, N08924S,
904L Stainless Steel Tube Price

TP904L Nerjaveèi Tib Espesifikasyon

SS Tib Spesifikasyon ASTM A213, ASME SA213
OD 1/8 "(3.18mm) OD a 5" OD (127mm)
Epesè 0.38mm – 12.7mm
Longè Single Random, Double Random & Longè Obligatwa
Fen Plain Fen, Bizote Fen, Treaded
Kondisyon livrezon Rekwit ak marinated, poli, klere rkwit, frèt trase
Anbalaj Chaje nan bwat an bwa, sache plastik, bann asye fourni, oswa selon demann kliyan yo
Espesyalis Gwosè ak espesifikasyon lòt pase sa ki anwo yo ka fabrike sou demann

Pri

5000-12000 USD / TÒN

Tan livrezon

7-45 jou

Kontakte kounye a

Nerjaveèi asye 904L Tib Pwopriyete mekanik

Dansite Pwen k ap fonn Fòs rupture Fòs Sede (0.2% Offset) Elongasyon
7.95 g/cm3 1350 degre (2460 degre F) Psi - 71000 , MPa - 490 Psi - 32000 , MPa - 220 35 %

 

ASME SA213 UNS N08904 Tib materyèl ekivalan

STANDARD WERKSTOFF NR. UNS JIS BS KS AFNOR EN
SS 904L 1.4539 N08904 SUS 904L 904S13 STS 317J5L Z2 NCDU 25-20 X1NiCrMoCu25-20-5

 

Gwosè Nominal Tiyo ⅛ a Gwosè Nominal Tiyo 3½

Gwosè tiyo nominal DN
mm
OD
pous (mm)
Epesè miray la
pous (mm)
SCH 5 SCH 10 SCH 30 SCH 40/STD SCH 80 SCH 120 SCH 160 XXS
⅛ 6 0.405 pous (10.29 mm) {{0}}}.035 pous (0.889 mm) 0.049 pous (1.245 mm) 0.057 pous (1.448 mm) 0.068 pous (1.727 mm) 0.095 pous (2.413 mm) - - -
¼ 8 0.540 pous (13.72 mm) 0.049 pous (1.245 mm) 0.065 pous (1.651 mm) 0.073 pous (1.854 mm) 0.088 pous (2.235 mm) 0.119 pous (3.023 mm) - - -
⅜ 10 0.675 pous (17.15 mm) 0.049 pous (1.245 mm) 0.065 pous (1.651 mm) 0.073 pous (1.854 mm) 0.091 pous (2.311 mm) 0.126 pous (3.200 mm) - - -
½ 15 0.840 pous (21.34 mm) 0.065 pous (1.651 mm) 0.083 pous (2.108 mm) - 0.109 pous (2.769 mm) 0.147 pous (3.734 mm) - 4.78mm 0.294 pous (7.47 mm)
¾ 20 1.050 pous (26.67 mm) 0.065 pous (1.651 mm) 0.083 pous (2.108 mm) 2.41mm 0.113 pous (2.870 mm) 0.154 pous (3.912 mm) - 5.56mm 0.308 pous (7.823 mm)
1 25 1.315 pous (33.40 mm) 0.065 pous (1.651 mm) 0.109 pous (2.769 mm) 2.90mm 0.133 pous (3.378 mm) 0.179 pous (4.547 mm) - 6.35mm 0.358 pous (9.093 mm)
1¼ 32 1.660 pous (42.16 mm) 0.065 pous (1.651 mm) 0.109 pous (2.769 mm) 0.117 pous (2.972 mm) 0.140 pous (3.556 mm) 0.191 pous (4.851 mm) - 6.35mm 0.382 pous (9.703 mm)
1½ 40 1.900 pous (48.26 mm) 0.065 pous (1.651 mm) 0.109 pous (2.769 mm) 0.125 pous (3.175 mm) 0.145 pous (3.683 mm) 0.200 pous (5.080 mm) - 7.14mm 0.400 pous (10.160 mm)
2 50 2.375 pous (60.33 mm) 0.065 pous (1.651 mm) 0.109 pous (2.769 mm) 0.125 pous (3.175 mm) 0.154 pous (3.912 mm) 0.218 pous (5.537 mm) 0.250 pous (6.350 mm) 8.74mm 0.436 pous (11.074 mm)
2½ 65 2.875 pous (73.02 mm) 0.083 pous (2.108 mm) 0.120 pous (3.048 mm) 0.188 pous (4.775 mm) 0.203 pous (5.156 mm) 0.276 pous (7.010 mm) 0.300 pous (7.620 mm) 0.344 pous (8.738 mm) 0.552 pous (14.021 mm)
3 80 3.500 pous (88.90 mm) 0.083 pous (2.108 mm) 0.120 pous (3.048 mm) 0.188 pous (4.775 mm) 0.216 pous (5.486 mm) 0.300 pous (7.620 mm) 0.350 pous (8.890 mm) 0.438 pous (11.13 mm) 0.600 pous (15.240 mm)
3½ 90 4.000 pous (101.60 mm) 0.083 pous (2.108 mm) 0.120 pous (3.048 mm) 0.188 pous (4.775 mm) 0.226 pous (5.740 mm) 0.318 pous (8.077 mm) - - 0.636 pous (16.154 mm)

 

ASTM A213 estanda tolerans dimansyon

Estanda Dyamèt ekstèn (mm) Epesè miray (mm) Longè (mm)
Range Devyasyon Range Devyasyon Range Devyasyon
ASTM A213 D<25.4 0.1/-0.1 D Mwens pase oswa egal a 38.1 20%/0 D<50.8;L mwens pase oswa egal a 7.3m 3/0
[25.4, 38.1] 0.15/-0.15
(38.1, 50.8) 0.2/-0.2
[50.8, 63.5) 0.25/-0.25 D>38.1 22%/0 D Pi gran pase oswa egal a 50.8;L Mwens pase oswa egal a 7.3m 5/0
[63.5, 76.2) 0.3/-0.3
[76.2, 101.6] 0.38/-0.38
(101.6, 190.5] 0.38/-0.64
(190.5, 228.6] 0.38/-1.14

 

ASTM A213 904L Nerjaveèi Tib Tretman Chalè:

SS 904L Tib se chalè trete nan 1090 degre a 1175 degre ki te swiv pa refwadisman rapid (anjeneral dlo trempe).

 

Aplikasyon nan ASTM A213 SS 904L Tib:

  • Asid silfirik, asid fosfò, plant pwosesis asid acetic
  • Ekipman refwadisman dlo lanmè
  • Kaka ak pwosesis papye
  • Konpozan rafineri
  • Transpò likid, gaz ak lwil oliv
  • Presyon ak transfè chalè
  • Chodyèr ak echanjeur chalè
  • Endistri chimik
  • Endistri lwil oliv ak gaz

 

FAQ

K: KonsènanASTM A213 904L Tib asye purpri?

A: Pri soti nan chenn $ 5 a $ 10 pou chak kilogram, varye selon gwosè, epesè miray, founisè elatriye.

K: Konbyen tan tan livrezon ou pran?

A: Tan livrezon se nan 5-21 jou

K: Èske gen sèvis echantiyon?

A: Yo bay echantiyon yo gratis

K: Ki kantite minimòm lòd?

A: Pa gen Kantite Lòd Minimòm

K: Ki jan yo pake pwodwi yo?

A: Kouch enteryè a gen yon kouch ekstèn papye ki enpèmeyab epi li fiks ak yon palèt an bwa fumigasyon.

K: Peyi ekspòte yo

A: Brezil, Lafrik di sid, Endonezi, peyi Zend, Singapore, Malezi, Iran, Larisi, UAE, Chili, Laos, elatriye

 

 

Baj popilè: 904l tib asye pur, astm a213 tib, 904l asye pur

Voye rechèch

whatsapp

Telefòn

Mel

Rechèch