ASTM A312 TP304L Nerjaveèi asye tiyo
1. estanda: ASTM A312 / ASME SA312
2. Gwosè: 1/8"- 30" (10.3-762mm)
3. Epesè: 0.5mm-30mm
4. Longè: Single, Double Random & Koupe Longè
ASTM A312 TP304L Nerjaveèise yon varyant ki ba kabòn nan kalite 304 asye pur. TP304L Nerjaveèi gen yon kontni maksimòm kabòn nan 0.03% pou pi bon rezistans nan korozyon intergranular, epi tou li gen yon minimòm de 18% CHROMIUM ak 8% nikèl.SS 304l tiyogen ekselan rezistans korozyon, rezistans tanperati ki wo, ekselan fòs ak rezistans serye, epi tou li gen bon plastisit ak soudabilite. Materyèl S30403 apwopriye pou pharmaceutique, chimik, lwil oliv ak gaz ak lòt aplikasyon ki sansib pou anviwònman an.
ASTM A312 304L estanda tiyo asye pur:
- ASTM A312: Espesifikasyon estanda pou tiyo asye pur san pwoblèm, soude, ak lou travay frèt.
- Klas ki disponib: TP304, TP304L, TP316, TP316L, 316Ti, TP317, TP317L, TP310, TP310S, TP321, TP347, TP347H, S31254, N08367, N08367
- ASME B36.19: Spesifikasyon pou tiyo asye pur

ASTM A312 TP304L Nerjaveèi asye tiyo Espesifikasyon
| Espesifikasyon |
ASTM A 312 ASME SA 312 |
| Dimansyon |
DIN, JIS, ASTM, GB, ASME, AISI, AMS, EN, GOST |
| SS 304L Tiyo | 1/2″ NB – 16″ NB |
| ERW 304L Tiyo | 1/2″ NB – 24″ NB |
| EFW 304L Tiyo | 6″ NB - 100″ NB |
| Gwosè | 1/8″NB POU 30″NB NAN |
| Orè | SCH5, SCH20, SCH40, STD, SCH60, SCH80, XS, SCH120, SCH140, SCH160, XXS |
| Kalite | San pwoblèm / ERW / soude / fabrike / LSAW Tiyo |
| Fòm | Tiyo wonn, tiyo koutim, tiyo kare, tiyo rektangilè, fòm "U", tiyo idwolik |
| Tretman andigman |
|
Konpozisyon chimik ASTM A312 Gr TP 304l Tiyo
- Kabòn: Mwens pase oswa egal a 0.035%
- Silisyòm: Mwens pase oswa egal a 1.00%
- Manganèz: Mwens pase oswa egal a 2.00%
- Fosfò: Mwens pase oswa egal a 0.045%
- Souf: Mwens pase oswa egal a 0.030%
- Kwòm: 18.0-20.0%
- Nikèl: 8.0-13.0%
SS UNS S30403 Pwopriyete mekanik tiyo
- Fòs rupture: ant 485 ak 515 MPa.
- Fòs sede: pa mwens pase 170 MPa.
- Elongasyon: pa mwens pase 35%
- Dite: Ranje dite komen yo se HRB 80-90 (dite Rockwell B) oswa HB 180-200 (dite Brinell).
- Dansite: 7.93 (g/cm³)
- Koefisyan ekspansyon tèmik: 17.2-18.2 (10⁻⁶/ degre , 20-100 degre )
ASTM A312 Enspeksyon Kalite
- Tès dite
- Tès aplati
- Tès korozyon pitting
- Chimik analiz - Spectral analiz
- Tès mikwo ak makro
- Tès fize
- Tès Kowozyon Entègranulèr (IGC).
- Tansyon zòn ak lòt tès mekanik
- Idantifikasyon fyab materyèl - Tès PMI
AISI 304L Nerjaveèi asye tiyo ekivalan materyèl klas
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | AFNOR | EN |
| SS 304L | 1.4306 / 1.4307 | S30403 | SUS 304L | 3304S11 | Z3CN18‐10 | X2CrNi18-9 / X2CrNi19-11 |
Alloy 304L Nerjaveèi asye Tablo dimansyon tiyo
|
Nominal |
Deyò |
Orè |
||||||||
|
5S |
10S |
40S |
80S |
|||||||
|
(mm) |
(pous) |
Mi epesè ak pwa |
||||||||
|
mm |
kg/m |
mm |
kg/m |
mm |
kg/m |
mm |
kg/m |
|||
|
1/8 |
10.3 |
0.405 |
- |
- |
1.25 |
0.28 |
1.73 |
0.37 |
2.42 |
0.47 |
|
1/4 |
13.7 |
0.540 |
- |
- |
1.66 |
0.49 |
2.24 |
0.63 |
3.03 |
0.80 |
|
3/8 |
17.2 |
0.675 |
- |
- |
1.66 |
0.63 |
2.32 |
0.85 |
3.20 |
1.10 |
|
1/2 |
21.3 |
0.840 |
1.65 |
0.81 |
2.11 |
1.00 |
2.77 |
1.27 |
3.74 |
1.62 |
|
3/4 |
26.7 |
1.050 |
1.65 |
1.02 |
2.11 |
1.28 |
2.87 |
1.68 |
3.92 |
2.20 |
|
1 |
33.4 |
1.315 |
1.65 |
1.30 |
2.77 |
2.09 |
3.38 |
2.50 |
4.55 |
3.24 |
|
1 1/4 |
42.2 |
1.660 |
1.65 |
1.66 |
2.77 |
2.69 |
3.56 |
3.39 |
4.86 |
4.47 |
|
1 1/2 |
48.3 |
1.900 |
1.65 |
1.91 |
2.77 |
3.11 |
3.69 |
4.06 |
5.08 |
5.41 |
|
2 |
60.3 |
2.375 |
1.65 |
2.40 |
2.77 |
3.93 |
3.92 |
5.45 |
5.54 |
7.49 |
|
2 1/2 |
73.0 |
2.875 |
2.11 |
3.69 |
3.05 |
5.26 |
5.16 |
8.64 |
7.01 |
11.4 |
|
3 |
88.9 |
3.500 |
2.11 |
4.52 |
3.05 |
6.46 |
5.49 |
11.3 |
7.62 |
15.3 |
|
3 1/2 |
101.6 |
4.000 |
2.11 |
5.18 |
3.05 |
7.41 |
5.74 |
13.6 |
8.08 |
18.6 |
|
4 |
114.3 |
4.500 |
2.11 |
5.84 |
3.05 |
8.37 |
6.02 |
16.1 |
8.56 |
22.3 |
|
5 |
141.3 |
5.563 |
2.77 |
9.46 |
3.41 |
11.6 |
6.56 |
21.8 |
9.53 |
31.0 |
|
6 |
168.3 |
6.625 |
2.77 |
11.3 |
3.41 |
13.9 |
7.12 |
28.3 |
10.98 |
42.6 |
|
8 |
219.1 |
8.625 |
2.77 |
14.8 |
3.76 |
20.0 |
8.18 |
42.5 |
12.70 |
64.6 |
|
10 |
273.1 |
10.750 |
3.41 |
22.7 |
4.20 |
27.8 |
9.28 |
60.4 |
12.70 |
81.5 |
|
12 |
323.9 |
12.750 |
3.97 |
31.3 |
4.58 |
36.1 |
9.53 |
73.9 |
12.70 |
97.4 |
ASTM A312 Mi Tolerans epesè
| NPS Designator | WT Tolerans, % soti nan Nominal | |
| Plis pase | Anba | |
| 1/8 a 2 1/2 enkli, tout rapò t/D | 20.0 | 12.5 |
| 3 a 18 incl., t/D jiska 5% incl. | 22.5 | 12.5 |
| 3 a 18 enkli, t/D > 5% | 15.0 | 12.5 |
| 20 ak pi gwo, soude, tout rapò t/D | 17.5 | 12.5 |
| 20 ak pi gwo, san pwoblèm, t/D jiska 5% incl. | 22.5 | 12.5 |
| 20 ak pi gwo, san pwoblèm, t/D > 5% | 15.0 | 12.5 |
- t=Epesè Mi Nominal
- D=Dyamèt deyò kòmande
FAQ
K: Konsènan pri tiyo asye pur ASTM A312 TP304L?
K: Konbyen tan tan livrezon ou pran?
K: Èske gen sèvis echantiyon?
K: Ki kantite minimòm lòd?
K: Ki jan yo pake pwodwi yo?
K: Peyi ekspòte yo
Baj popilè: 304l tiyo asye pur, astm a312 tp304l, tiyo 304l, tiyo asye pur 304l
Ou ka renmen tou
Voye rechèch