Monel UNS N05500 Tiyo

Monel UNS N05500 Tiyo


1. estanda: ASTM B165, ASTM B163, ASTM B829, ASTM B725
2. OD gwosè: 6.35 milimèt pou 254 milimèt
3. pesè: SCH5 ~ SCHXXS
4. Ekivalan: UNS N05500, Din 2.4375, Monel K500
Voye rechèch
Pwodwi Entwodiksyon

Monel UNS N05500 Tiyo (Werkstoff Nr. 2.4375)te sòti nan Monel 400 ak aliminyòm ak Titàn te ajoute pou laj redi, li karakteristik ranfòse fòs ak dite pandan y ap kenbe ekselan rezistans korozyon, lajman ki itilize nan pwosesis chimik, lwil oliv ak gaz, jeni maren ak espas aeryen. HT PIPE se yonMonel k500 tiyofounisè ki gen 15+ eksperyans ekspòtasyon.Kontakte noupou plis enfòmasyon ak quotes gratis!

Nou ofri Monel UNS N05500 nan yon varyete fòm, tankou:

  • Bar
  • Fil
  • Fèy
  • Plak
  • Forgings
  • Fittings tiyo
  • Bride
  • Tiyo san pwoblèm & soude
  • Tib san pwoblèm & Tib soude
  • Weld Rod
monel uns n05500 pipe

Espesifikasyon Tib Monel K500

Espesifikasyon

ASTM B165, ASTM B163, ASTM B829, ASTM B725

Dimansyon ASTM, ASME, ak API
OD 6.35 mm OD jiska 254 mm OD
WT 0.6 mm POU 20 mm
Kalite San pwoblèm / EFW / ERW / soude / fabrike
Fòm Wonn, idwolik elatriye
Longè Single Random, Double Random & Koupe Longè.
Fen Plain Fen, Bizote Fen, Treaded

Kontakte kounye a

K500 Monel Round Tiyo Chimik Konpozisyon

Monel K500 Ni C Al Mn Si Fe Cu S Ti Kr
63.0 min 0.25 max 2.3 – 3.15 1.5 max 0.5 max 05 – 2 27.0 – 33.0 0.010 max 0.35 – 0.85

 

Pwopriyete fizik Monel K500 tiyo

dansite 8.44 g/cm³, pwen k ap fonn 1315 -1350 degre, konduktiviti tèmik 40 W/(m·K), rezistivite elektrik 90 μΩ·cm, modil Young 179 GPa, rapò Poisson a 0.32. Ki pa mayetik pi wo a -200 degre, kenbe duktilite ak severite nan -400 degre.

 

alyaj k500 tiyo Pwopriyete mekanik

fòs rupture 1100 MPa (160000 psi), fòs sede (0.2% konpanse) 790 MPa (115000 psi), elongasyon 20%. De fwa fòs rupture ak twa fwa fòs sede Monel 400, kenbe fòs jiska 648 degre (1200 degre F).

 

Monel K500 Tib gwosè ak pwa

Dimansyon Mi Pwa pou chak Dimansyon Mi Pwa pou chak
(mm) (mm) mèt (kg) (mm) (mm) mèt (kg)
12.7 x 12.7 1.20 0.44 40 x40 1.20 1.49
12.7 x 12.7 1.50 0.55 40 x40 1.50 1.85
15 x 15 1.20 0.53 40 x40 2.00 2.45
15 x 15 1.50 0.65 40 x40 3.00 3.75
20 x 20 1.20 0.71 50 x50 1.50 2.32
20 x 20 1.50 0.88 50 x50 2.00 3.08
20 x 20 2.00 1.19 50 x50 3.00 4.65
25 x 25 1.20 0.92 60 x60 2.00 3.71
25 x 25 1.50 1.14 60 x60 3.00 5.49
25 x 25 2.00 1.49 70 x70 3.00 6.53
25 x 25 3.00 2.20 80 x80 2.00 4.98
30 x 30 1.20 1.10 80 x80 3.00 7.53
30 x 30 1.50 1.37 100 x 100 2.00 6.40
30 x 30 2.00 1.84 100 x 100 3.00 9.53

 

FAQ

K: Konsènan pri tiyo Monel UNS N05500?

A: Pri soti nan chenn $30 - $35 pou chak kilogram, varye selon gwosè, epesè miray, founisè elatriye.

K: Konbyen tan tan livrezon ou pran?

A: tan livrezon se nan 5-21 jou

K: Èske gen sèvis echantiyon?

A: Yo bay echantiyon yo gratis

K: Ki kantite minimòm lòd?

A: Pa gen Kantite Lòd Minimòm

K: Ki jan yo pake pwodwi yo?

A: Kouch enteryè a gen yon kouch ekstèn papye ki enpèmeyab epi li fiks ak yon palèt an bwa fumigasyon.

K: Peyi ekspòte yo

A: Brezil, Lafrik di sid, Endonezi, peyi Zend, Singapore, Malezi, Iran, Larisi, UAE, Chili, Laos, elatriye

K: Èske nou ka vizite faktori ou a?

A: Natirèlman, ou toujou akeyi!

 

 

 

Baj popilè: monel uns n05500 tiyo, Lachin monel uns n05500 tiyo manifaktirè, alyaj k500 tiyo founisè, uns n05500 tib pri

Voye rechèch

whatsapp

Telefòn

Mel

Rechèch