Tolerans tiyo ki espesifye pa ASME B36.10/36.19
Tolerans dyamèt tiyo
| PIPE NPS/ DN/ OD | Tolerans dyamèt deyò ki pèmèt | |||
|---|---|---|---|---|
| Plis pase | Anba | |||
| pous | mm | pous | mm | |
| NPS 1/8 a 1½ DN 6 a 40 OD 10.3 pou 48.3, milimèt |
1/64 | 0.4 | 1/64 | 0.4 |
| Plis pase 1½ a 4 DN 40 a 100 OD 48.3 a 114.3 mm |
1/32 | 0.8 | 1/32 | 0.8 |
| Plis pase 4 a 8 DN 100 a 200 OD 114.3 a 219.1 mm |
1/16 | 1.6 | 1/32 | 0.8 |
| Plis pase 8 a 18 DN 200 a 450 OD 219.1 a 457 mm |
3/32 | 2.4 | 1/32 | 0.8 |
| Plis pase 18 a 26 DN 450 a 650 OD 457 a 660 mm |
1/8 | 3.2 | 1/32 | 0.8 |
Tolerans epesè tiyo
| PIPE NPS/ DN/ OD | Tolerans, % soti nan Nominal | |
|---|---|---|
| Plis pase | Anba | |
| NPS 1/8 a 2½, tout rapò t/D DN 6 a 65 OD 10.3 a 73.0, mm |
20.0 | 12.5 |
| NPS 3 a 18, t/D jiska 5% DN 80 a 450 OD 88.9 a 457 mm |
22.5 | 12.5 |
| NPS 3 a 18, t/D > 5% DN 80 a 450 OD 88.9 a 457 mm |
15.0 | 12.5 |
| NPS 20 ak pi gwo, soude, tout rapò t/D DN 500 OD 508 mm |
17.5 | 12.5 |
| NPS 20 ak pi gwo, san pwoblèm, t/D jiska 5% DN 500 OD 508 mm |
22.5 | 12.5 |
| NPS 20 ak pi gwo, san pwoblèm, t/D > 5% DN 500 OD 508 mm |
15.0 | 12. |
Tolerans longè tiyo
- Sans ak soude (pa gen okenn metal ajoute): si longè koupe yo bay lòd, pa gen okenn longè tiyo ki dwe anba longè ki espesifye a epi yo pa dwe plis pase 1/4 pous (6.35 mm) sou sa ki espesifye.
- Fòje ak anwiye, jete, ak jete frèt-fòje: si longè koupe definitif yo bay lòd, pa gen okenn longè tiyo a dwe anba longè espesifye a epi yo pa dwe plis pase 1/8 pous (3.2 mm) sou sa ki espesifye.
- Poutiyo asye puròdone longè o aza, longè ak varyasyon yo dwe dakò ant manifakti a ak achtè a
Tolerans pwa tiyo
Tolerans pwa tiyo yo depann de gwosè nominal tiyo a, jan lis anba a:
- Tiyo NPS 4 (DN100, 114.3mm) ak pi piti yo ka peze nan anpil pratik; tiyo nan gwosè ki pi gwo pase NPS 4 dwe peze separeman
- Tiyo NPS 12 (DN300, 323.8mm) ak anba, tolerans pwa se: -3.5% / +10%
- Tiyo sou NPS 12 (DN300, 323.8mm), tolerans pwa se: -5% / +10%
Tolerans kantite tiyo
Ta dwe nan -10% to +10% tolerans, kòm yon règ (-3/+3% ta dwe akseptab)