Super Duplex 2507 Datasheet
ASTM A789 UNS S32750 TIB contains 25% chromium, 4% molybdenum and 7% nickel. The high molybdenum, chromium and nitrogen content makes it highly resistant to chloride pitting and crevice corrosion, and the PREN (pitting resistance equivalent) of UNS S32750 is >{{0}}.0, ki asire gwo rezistans pitting. Segondè fòs mekanik (tipikman jiska 570 MPa fòs sede), ak estrikti san pwoblèm gen pi gwo presyon pote kapasite pase soude.

Konpayi fabrikasyon Founisè SCH 40S Super Duplex Tubing, SDSS Enstriman Tib ak SAF 2507 Tib dapre ASME B36.19 ak ASTM A789, Gade dimansyon gwosè nou yo ak pri
| Epesè | 0.3mm – 50mm, SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS |
| Dyamèt Eksteryè | 6.00 mm OD jiska 914.4 mm OD, gwosè jiska 24" NB, Customized |
| ASTM A789 UNS S32750 Pri | USD 10-15 pou chak kg |
Super Duplex 2507 Tib Tanperati Range
- Yo mete aksan espesyal souSuper Duplex 2507 Tibpwodui dapre espesifikasyon ASTM A789, paske li gen tandans vin frajil anba ekspoze pwolonje nan tanperati ki pi wo a 600 degre F.
- Manifaktirè devwe nou yo fè analiz tretman chalè osi byen ke tès mekanik sou Alloy 2507 pou tcheke si li satisfè spesifikasyon an.
Aplikasyon nan ASTM A789 UNS S32750 Super Duplex Nerjaveèi Tib
- Endistri Pwosesis Chimik
- Endistri marin ak konstriksyon bato: Propellers ak arbr, gouvernay, sele arbr, ponp, boulon ak fixation, tiyo, instrumentation, tankers ak gaz chimik.
- Endistri lwil oliv ak gaz: Ponp, Tiyo, Tiyo, Veso, Ekipman Wellhead, Ekipman Subsea
- Kontwòl polisyon: fanatik ak ponp, épurateur mouye, ensinerateur, tretman dlo egou
- Endistri kaka ak papye: Tib aparèy chofaj likè nwa, tiyo soufle dijester, tiyo manje rotary, rondelles stock mawon, kolon, konpozan blanchi.