Dec 31, 2024 Kite yon mesaj

2025 SS 904L Pri|Plak tiyo Bar bride Fittings

SS 904L plak pri pou chak kilogram

Kòm nan 2025, pri a nan904L plak asye purtipikman varye ant $5.50 ak $6.50 pou chak kg. Pri yo ka varye selon epesè plak, gwosè, ak kantite lòd.

 

SS 904L Tiyo Pri Pa Kilogram

ASTM A312 SS 904L tiyo san pwoblèm oswa soude koute tipikman ant $ 6.00 ak $ 7.50 pou chak kg. Pri varye selon faktè tankou dyamèt tiyo, epesè miray, ak longè.
 

SS 904L Round Bar Pri pou chak kg

Ba wonn asye pur 904L, pri anjeneral varye ant $6.00 rive $7.00 pou chak kg. Pri ka varye selon si wi ou non ba a se wonn, kare oswa egzagonal, osi byen ke longè ak dyamèt ba a.

 

SS 904L Flange Pri pou chak kg

Pri tipik pou bride asye pur 904L varye ant $8.00 rive $9.50 pou chak kg. Pri flange yo afekte pa faktè tankou kalite bride (egzanp, kou soude, slip-on, threaded, priz, avèg), gwosè, ak konpleksite nan konsepsyon koutim.

 

SS 904L Fittings Pri pou chak kg

Fittings SS 904L, ki gen ladan koud, tees, redukteur, ak kouple. Pri fitting Alloy 904L anjeneral varye ant $7.00 rive $8.50 pou chak kg.

 

Faktè ki afekte pri alyaj 904L:

  • Pri materyèl bwit: Pri nikèl, molybdène ak lòt matyè premyè kontwole pri asye 904l.
  • Defi chèn ekipman pou: depans transpò, tarif entènasyonal yo ak faktè jeopolitik.
  • Pwosesis fabrikasyon (tankou gwosè koutim oswa kouch espesyal) ka chanje pri.

 