SS 904L Tiyo
1. estanda: ASTM A312, ASME SA312, ASTM A269, ASTM A213, ASTM B677
2. gwosè: 1/2''~48''
3. pesè: SCH5 ~ SCHXXS
4. Sèvis: koupe, soude, fabrike, Customized
5. Klas: Alloy 904l, UNS N08904, en 1.4539
ASTM A312 TP 904L Tiyo Founisè nan Lachin
SS 904L Tiyokonsiste de chromium, nikèl ak kwiv. Copper yo ajoute nan alyaj 904L Nerjaveèi asye a, Se poutèt sa, li trè rezistan a asid rediksyon fò tankou asid silfirik. Kontni kabòn ki pi ba a fè tiyo soude AISI 904L pi fasil.ASTM 904Lse sitou itilize pou aplikasyon jeneral korozyon.
TP 904L Nerjaveèi asye tiyo san pwoblèm valè te ajoute sèvis
- Polisaj
- Bizote
- Personaj/Vire
- Heatreaating & Recuit
- Idantifikasyon materyèl pozitif (PMI)
- Tès UT

Spesifikasyon Lis SS 904L Tiyo
| Espesifikasyon | ASTM A312, ASTM A269, ASTM A213, ASTM B673, B677 |
|---|---|
| Dimansyon | ASTM, ASME ak API |
| SS 904 L Tiyo | 1/2% e2�� NB – 16% e2�� NB |
| ERW 904L Tiyo | 1/2% e2�� NB – 24% e2�� NB |
| EFW 904L Tiyo | 6″ NB - 100″ NB |
| Gwosè | 1/8″NB POU 30″NB NAN |
| Espesyalize nan | Gwo dyamèt gwosè |
| Orè | SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60% 2c SCH80, SCH120, SCH140, SCH160, XXS |
| Kalite | San pwoblèm / ERW / soude / fabrike / LSAW Tiyo |
| Fòm | Wonn, kare, rektangilè, idwolik elatriye |
| Longè | Single Random, Double Random & Koupe Longè. |
| Fen | Plain Fen, Bizote Fen, Treaded |
Nerjaveèi asye 904L Tiyo Presyon Rating
| TANPERATI | KONPARASON AK LÒT TIPO TANPERATI GWO | |||
|---|---|---|---|---|
| degre F | degre | ALYAJ 254 | TIP 904L | ALYAJ 825 |
| 200 | 93 | 0.88 | 0.82 | 1.00 |
| 300 | 149 | 0.79 | 0.74 | 0.95 |
| 400 | 204 | 0.73 | 0.68 | 0.90 |
| 500 | 260 | 0.69 | 0.63 | 0.87 |
| 600 | 315 | 0.66 | 0.58 | 0.84 |
| 700 | 371 | 0.64 | 0.56 | 0.81 |
| 800 | 426 | 0.79 | ||
SB 677 UNS N08904 Pwopriyete mekanik tiyo san pwoblèm
- Fòs Sede se 220MPa
- Fòs rupture se 490MPa
- Rockwell B Hardness Grade se tou 70-90
AISI904L Nerjaveèi asye san pwoblèm ak tiyo ERW
Tiyo SS 904L ki gen ladan tiyo san pwoblèm ak soude (ERW, EFW, SAW) yo te fè nan alyaj nikèl-chromium ak pi ba kontni kabòn.904L asye pur tiyo san pwoblèmgen gwo presyon pote kapasite, gwo-dyamèt tiyo soude gen pri ki ba, apwopriye pou gwo koule likid nan lwil oliv ak gaz, ak efikasite segondè.
904l Nerjaveèi asye san pwoblèm tès tiyo
Dapre ASTM A312, chak904l tibyo dwe apwovizyone nan eta chalè-trete ak tanperati tretman chalè apwopriye ak refwadisman ak tès.
- Tès tansyon transverse oswa longitudinal
- Tès aplati
- Tès ki pa destriktif
- X-ray deteksyon defo
- Tès rezistans korozyon
- Tès presyon idwolik
- À
FAQ
K: Konsènan pri alyaj 904l asye pou chak kg?
K: Konbyen tan tan livrezon ou pran?
K: Èske gen sèvis echantiyon?
K: Ki kantite minimòm lòd?
K: Ki jan yo pake 1.4539 aisi 904l pwodwi yo?
K: Peyi ekspòte yo