S17400 Nerjaveèi asye tiyo
1.Standard: ASTM A705, ASTM A693, ASTM A564, AMS 5643
2.Gwosè: 1/8"- 48"
3.Epesè: 0.4mm jiska 30.00 mm
4.Length: Single, Double Random & Koupe Longè
S17400 tiyo asye purse yon kalite presipitasyon-redi Nerjaveèi asye ki rele tou17-4 PHoswaASTM A564 Kalite 630. Li gen chromium, nikèl, ak kwiv kòm eleman alyaj prensipal yo, ak adisyon nan molybdène, niobyòm, ak Tantal pou amelyore rezistans korozyon, severite, ak travayabilite.SUS 630 enka kenbe tèt ak tanperati ki wo jiska 593 degre san deformation enpòtan oswa oksidasyon.1.4542 asye purka transfòme soti nan yon eta mou ak duktil nan yon eta difisil ak fò atravè pwosesis tretman chalè senp.
Nerjaveèi 17-4PH TiyoZòn aplikasyon:
- Aerospace
- Endistri chimik
- Réacteurs, tank depo, tuyaux
- Lwil oliv ak gaz
- Aparèy Medikal

Nerjaveèi 17-4 PH Tiyo Spesifikasyon:
| Kalite | Tiyo san pwoblèm, tiyo soude, tiyo ERW, tiyo EFW, tiyo LSAW, tiyo fabrike |
| Klas | SS 17-4 PH / UNS S17400 / 1.4542 / SUS 630 |
| Fòm | Tiyo kare, tiyo wonn, tiyo rektangilè, tiyo soude, tiyo san pwoblèm, tiyo EFW, tiyo ERW, tiyo idwolik, tiyo oval, tiyo poli, tiyo fabrike, elatriye. |
| Estanda | ASTM A312, ASME SA312 / ASTM A358, ASME SA358 / AMS 5643 |
| Orè | SCH 5S, SCH 10S, SCH 20, SCH 40S, SCH 160S, SCH 60, SCH 80, SCH 120, SCH XS, SCH XXS, elatriye (PI LWA SOU DEMANN) |
| Gwosè Range | 1/8″ NB Pou 48″ NB |
| Longè | Single o aza, doub o aza, koupe longè. |
| Fen tiyo | Plain Fen, Treaded, Bizote Fen |
| Sifas fini | No.1 fini, 2B fini, No.8 glas fini, No.4 fini |
Tib PH asye pur 17-4& Tiyo Pwopriyete mekanik
| Pwopriyete | Metrik / Imperial |
| Dansite | 7.75 g/cm3 / 0.280 lb/in3 |
SS 17-4 1.4542 AISI 630 Dansite:
| Kondisyon | Dansite |
|---|---|
| Kond A | 0.280 #/pous3 |
| Kond H900 | 0.282 #/pous3 |
| Kond H1075 | 0.283 #/pous3 |
| Kond H1150 | 0.283 #/pous3 |
17-4 Nerjaveèi AMS 5643 Dite ak Pwopriyete Minimòm Tensil:
Pou dyamèt 8" ak pi ba a (oswa pi piti distans ant kote paralèl yo)
| Kondisyon | Tensile | Sede 0.2% konpanse | Elongasyon (% nan 2") | Rediksyon nan zòn | Brinell dite | Rockwell dite |
|---|---|---|---|---|---|---|
| H900 | 190 ksi | 170 ksi | 10% | 40% (35% >3") | 388-444 HB | 40-47 HRC |
| H925 | 170 ksi | 155 ksi | 10% | 44% (38% >3") | 375-429 HB | 38-45 HRC |
| H1025 | 155 ksi | 145 ksi | 12% | 45% | 331-401 HB | 34-42 HRC |
| H1075 | 145 ksi | 125 ksi | 13% | 45% | 311-375 HB | 31-38 HRC |
| H1100 | 140 ksi | 115 ksi | 14% | 45% | 302-363 HB | 30-37 HRC |
| H1150 | 135 ksi | 105 ksi | 16% | 50% | 277-352 HB | 28-37 HRC |
| Ann | - | - | - | - | 363 max | 39 HRC Max |
FAQ
K: Ki pri S17400 Nerjaveèi a?
K: Èske li nan stock?
K: Èske gen sèvis echantiyon?
K: Ki kantite minimòm lòd?
K: Konbyen tan tan livrezon an?
K: Ki metòd peman yo sipòte?
K: Èske ou bay sètifika tès faktori?
K: Èske ou sipòte pwodwi Customized?
Baj popilè: s17400 asye pur, s17400 tiyo asye pur, S17400 tiyo
Ou ka renmen tou
Voye rechèch