N08904 Nerjaveèi asye tiyo
,1. Estanda: ASTM A312, ASME SA312
,2. Gwosè: 1/2''~48''
,3. Epesè: SCH5 ~ SCHXXS
,4. Sèvis: Koupe, soude, fabrike, Customized
N08904 Nerjaveèi asye tiyose yon klas super austenitic ak 19% a 23% chromium, 23% a 28% nikèl ak 4-5% molybdène. Tib Alloy 904L gen ekselan rezistans nan medya korozivite ak diminye.ASTM A213 TP904L tibka itilize jiska 400 degre Sèlsiyis nan prezans asid silfirik dilye. Solisyon manifaktirè nou yo chalè trete ak woulo liv frèt nan 1090 a 1175 degre Sèlsiyis. Tiyo soude se pi bon mache epi li pran mwens tan nan pwosesis pase tiyo san pwoblèm.
904L UNS N08904 Aplikasyon pou tiyo asye pur:
- Ekipman refwadisman dlo lanmè
- Pwosesis chimik nan asid silfirik, fosfò ak asid
- Endistri lwil oliv ak gaz
- Fwote gaz
- Tib kondansateur
- Echanjeur chalè

1.4539 AISI 904L NerjaveèiEspesifikasyon
| Espesifikasyon estanda | ASTM A312, ASTM A213, ASTM B677 |
| Kalite | ERW, san pwoblèm, soude, EFW |
| Estanda | DIN, JIS, AMS, GB, AISI, ASME, ASTM, EN, GOST |
| Gwosè | OD: 4 a 219mm OD: 5.0 - 1219.2 mm OD: 5.0 - 1219.2 mm |
| Orè epesè | SCH 10, SCH 40, SCH 80, SCH 5, SCH XS, SCH XXS, SCH 160, SCH 80S Founisè nan Mumbai |
| Sifas fini | Bright, Fwad Fini, Recuit, Poli, marinated |
| Teknik | Woule Fwad Woule cho |
| Epesè miray la | 0.1 Pou 60 mm |
| Teknoloji Faktori | Cho / Fwad Fòme |
ASTM A213 TP904L Tib Evalyasyon Presyon
| Tanperati, degre F | Btu/(lb degre F) | Tanperati, degre | J/(kg degre) |
|---|---|---|---|
| 200 | 0.12 | 100 | 485 |
| 68 | 0.11 | 20 | 460 |
| 1200 | 0.15 | 600 | 605 |
| 400 | 0.12 | 200 | 515 |
| 800 | 0.14 | 400 | 570 |
| 1300 | 0.15 | 700 | 615 |
| 600 | 0.13 | 300 | 545 |
| 1000 | 0.14 | 500 | 590 |
SS 904L VS 254SMO | 316L |304L
Rezistans korozyon nan 904L klas Nerjaveèi manti ant klas yo super austenitic ak kontni molybdène 6% ak estanda 316L klas austenitic la. EN 1.4539 klas 904L gen yon pi wo rezistans nan asid nitrique pase 304L san molybdène.
904L UNS N08904 Aplikasyon pou tiyo asye pur
- Ekipman refwadisman dlo lanmè
- Pwosesis chimik nan asid silfirik, fosfò ak asid
- Endistri lwil oliv ak gaz
- Fwote gaz
- Tib kondansateur
- Echanjeur chalè
FAQ
K: Konsènan pri SS 904L pou chak kg?
K: Konbyen tan tan livrezon ou pran?
K: Èske gen sèvis echantiyon?
K: Ki kantite minimòm lòd?
K: Ki jan yo pake pwodwi yo?
K: Peyi ekspòte yo
Baj popilè: n08904 asye pur, n08904 tiyo