ASTM A213 TP304 Steel Tib
1. estanda: ASTM A213, ASME SA213
2. OD gwosè: 6.0mm -114.0mm
3. Epesè miray la: 0.6mm -12.7mm
4. Ekivalan: UNS S30400, DIN 1.4301, AISI 304
ASTM A213 TP304 Steel Tibse sitou konpoze de fè, ak yon gwo kantite chromium (apeprè 18-20%) ak nikèl (apeprè 8-10.5%) te ajoute pou amelyore rezistans korozyon. Li genyen tou ti kantite lòt eleman tankou kabòn, Manganèz, Silisyòm, fosfò, souf ak nitwojèn.SS 304 Tibse li te ye pou ekselan rezistans korozyon li yo, rezistans oksidasyon ak fòs tanperati ki wo. Konpayi nou an se yon founisè tiyo asye pur ak eksperyans ekspòtasyon 15+, kontakte nou pou plis enfòmasyon ak sitasyon pi ba gratis!
ASTM A213 TP304 Estanda Tib asye pur:
-
ASTM A213: Spesifikasyon pou chodyè asye san pwoblèm feritik ak austenitic alyaj, surchofaj, ak tib echanjeur chalè.
- Klas Estanda Ameriken: TP304L, TP310S, TP316, TP316L, 316Ti, TP321, TP321H, TP317, TP317L, TP347, TP347H, 254SMO, AL6XN, 904L
- Klas estanda Ewopeyen an: 1.4301, 1.4306, 1.4961, 1.4547, 1.4539, 1.4401/1.4436, 1.4404/1.4435, 1.4571, 1.4449, 1.4449, 1.41.48, 1.41.48, 1.41. 1.4845, 1.4550

1.4301 304 Espesifikasyon Tib asye pur
|
Spesifikasyon |
ASTM A213 / ASME SA213 |
|
Dimansyon |
ASTM ak ASME |
|
Kalite |
San pwoblèm Ferritic ak Austenitic Chodyè, Superheat, ak Chalè-Echanjeur Tib |
|
Gwosè Dyamèt Eksteryè |
1/8 "OD, NB a 5" OD, NB gwosè |
|
Epesè |
0.4mm rive 12.7mm |
|
Longè |
Jiska 6 mèt, longè koutim koupe |
|
Fini |
No.1 Pickled Fini, No.4 fini, BA Fini, Electropolished tib san pwoblèm |
|
Kondisyon livrezon |
Kòm woule, fòme, soulaje estrès, rkwit, fè tèt di, apeze, trase frèt. |
Pwopriyete mekanik ASME SA213 UNS S30400:
- Minimòm fòs rupture: Pi gran pase oswa egal a 515MPa
- Fòs sede: Pi gran pase oswa egal a 205MPa
- Elongasyon: pi gran pase oswa egal a 35%
- Dite: Mwens pase oswa egal a 90HRB (Rockwell dite B)
Aplikasyon AISI 304 SS Steel tiyo
- Petrochimik
- Chimik
- Jenerasyon pouvwa
- Pwosesis endistriyèl
Faktori ASTM A213 UNS S30400 Tib
An tèm de pwodiksyon ak manifakti, TP304 Nerjaveèi asye tiyo san pwoblèm adopte pwosesis tanperati ki wo, epi li fèt nan pwosesis miltip tankou Distribisyon kontinyèl, woule, pèforasyon, tretman chalè, marinated, elatriye.
ASTM A213 304 Gwosè Tib asye pur
| OD AN POUS | KALIBÒM MI | MI DESIMAL | ID AN POUS | PWA POU FT. NAN LBS. |
| 1/4 | 20 | 0.035 | 0.18 | 0.08 |
| 1/4 | 18 | 0.049 | 0.152 | 0.105 |
| 1/4 | 16 | 0.065 | 0.12 | 0.128 |
| 5/16 | 16 | 0.065 | 0.183 | 0.172 |
| 3/8 | 20 | 0.035 | 0.305 | 0.127 |
| 3/8 | 16 | 0.065 | 0.245 | 0.215 |
| 1/2 | 20 | 0.035 | 0.43 | 0.174 |
| 1/2 | 18 | 0.049 | 0.402 | 0.236 |
| 1/2 | 16 | 0.065 | 0.37 | 0.302 |
| 1/2 | 13 | 0.095 | 0.31 | 0.411 |
| 5/8 | 18 | 0.049 | 0.527 | 0.301 |
| 5/8 | 16 | 0.065 | 0.495 | 0.389 |
| 5/8 | 11 | 0.12 | 0.385 | 0.647 |
| 3/4 | 20 | 0.035 | 0.68 | 0.267 |
| 3/4 | 16 | 0.065 | 0.62 | 0.476 |
| 3/4 | 13 | 0.095 | 0.56 | 0.665 |
| 7/8 | 11 | 0.12 | 0.635 | 0.968 |
| 1 | 20 | 0.035 | 0.93 | 0.361 |
| 1 | 18 | 0.049 | 0.902 | 0.498 |
| 1 | 16 | 0.065 | 0.87 | 0.649 |
| 1 | 14 | 0.083 | 0.834 | 0.813 |
| 1 | 11 | 0.12 | 0.76 | 1.128 |
| 1 | 1/4 | 0.25 | 0.5 | 2.003 |
| 1 1/4 | 16 | 0.065 | 1.12 | 0.823 |
| 1 1/4 | 11 | 0.12 | 1.01 | 1.448 |
| 1 1/4 | 3/16 | 0.188 | 0.874 | 2.132 |
| 1 1/4 | 1/4 | 0.25 | 0.75 | 2.67 |
| 1 1/2 | 16 | 0.065 | 1.37 | 0.996 |
| 1 1/2 | 11 | 0.12 | 1.26 | 1.769 |
| 1 1/2 | 1/4 | 0.25 | 1 | 3.338 |
| 1 3/4 | 11 | 0.12 | 1.51 | 2.089 |
| 2 | 16 | 0.065 | 1.87 | 1.343 |
| 2 | 11 | 0.12 | 1.76 | 2.409 |
| 2 | 3/16 | 0.188 | 1.624 | 3.638 |
| 2 | 1/4 | 0.25 | 1.5 | 4.673 |
| 2 1/4 | 3/16 | 0.188 | 1.874 | 4.14 |
| 2 1/4 | 1/4 | 0.25 | 1.75 | 5.34 |
| 2 1/2 | 11 | 0.12 | 2.26 | 3.05 |
| 2 1/2 | 1/4 | 0.25 | 2 | 6.008 |
| 3 | 11 | 0.12 | 2.76 | 3.691 |
| 3 | 3/16 | 0.188 | 2.624 | 5.646 |
| 3 | 1/4 | 0.25 | 2.5 | 7.343 |
304 Nerjaveèi asye Tib Deyò Tolerans Dyamèt
| Woule cho | Dyamèt deyò, mm | Tolerans, mm |
| OD Mwens pase oswa egal a 101.6 | 0.4/-0.8 | |
| 101.6<OD Mwens pase oswa egal a 190.5 | 0.4/-1.2 | |
| 190.5<OD Mwens pase oswa egal a 228.6 | 0.4/-1.6 | |
| Fwad trase | Dyamèt deyò, mm | Tolerans, mm |
| OD�% bc% 9c25.4 | ±0.10 | |
| 25.4 Mwens pase oswa egal a OD Mwens oswa egal a 38.1 | ±0.15 | |
| 38.1<OD<50.8 | ±0.20 | |
| 50.8 Mwens pase oswa egal a OD<63.5 | ±0.25 | |
| 63.5 Mwens pase oswa egal a OD<76.2 | ±0.30 | |
| 76.2 Mwens pase oswa egal a OD Mwens oswa egal a 101.6 | ±0.38 | |
| 101.6<OD Mwens pase oswa egal a 190.5 | 0.38/-0.64 | |
| 190.5<OD Mwens pase oswa egal a 228.6 | 0.38/-1.14 |
FAQ
K: Konsènan pri ASTM A213 TP304 Steel Tib?
K: Konbyen tan tan livrezon ou pran?
K: Èske gen sèvis echantiyon?
K: Ki kantite minimòm lòd?
K: Ki jan yo pake pwodwi yo?
K: Peyi ekspòte yo
Baj popilè: 304 tib asye, astm a213 tp304, 304 tib asye pur, 304 tib ss
Ou ka renmen tou
Voye rechèch