Dec 11, 2024 Kite yon mesaj

DN48 ASTM A815 UNS S32750 2507 Egal Tee Fittings

2507 Tee Egal San pwoblèm, ASTM A815, DN100, Tee Egal, SCH40S, SCH XS, Tee Egal San pwoblèm, 2507 Tee Egal San pwoblèm, UNS S32750 Tee Egal San pwoblèm

 

ASTM A815 UNS S32750 Super Duplex SS Egal Tee

1. Fwad Fòme
2. Materyèl: Super Duplex Nerjaveèi 2507 (F53 / 1.4410 / UNS S32750)
3. meyè kalite, konpetitif ba pri.

4. Ekspòtasyon: Fittings Super Duplex 2507 nou yo te ekspòte nan Etazini, Endonezi, Malezi, Brezil, Chili, Perou ak Mwayen Oryan an.

 

ASTM A815 UNS S32750 2507 Equal Tee Fittings

 

Super Duplex 2507 Materyèl

Super Duplex 2507 (F53 / 1.4410 / UNS S32750) gen ekselan rezistans korozyon ak ekselan rezistans nan pitting ak korozyon fant nan dlo lanmè ak lòt anviwònman klori. Tanperati kritik pitting se plis pase 50 degre. Koyefisyan ekspansyon tèmik la pi ba pase sa yo ki an asye austenitic, ak konduktiviti tèmik la pi wo, apwopriye pou travay tanperati jiska 300 degre. Nou bay touSuper Duplex 2507 tiyo, plak asye, ekipman tiyo, bride, elatriye.

 

Klas Chimi (valè tipik) Mekanik
Spesifikasyon Kr Ni Mo Cu N W Si Mn P
max
S
max
C
max
Fe UTS
N/mm²
(min)
0.20%
Prèv
(min)
Long
% (min)
Dite
HB (max)
PREN
2507 25.0 7.0 3.8 0.75 0.25 0.28 0.80 1.20 0.035 0.020 0.030 Bal 750 500-550 25 270 41

 

Kontakte nou pou plis enfòmasyon ak quotes gratis!

Kontakte kounye a

 

ASTM A815 UNS S32750 Butt Weld Fittings Sètifika Tès

  • EN 10204/3.1B
  • Sètifika Materyèl kri
  • Rapò tès radyografi 100%.
  • Rapò Enspeksyon Twazyèm Pati

 

 