ASTM A240 UNS S31700 Plak
1.Standard: ASTM A240, ASME SA240
2.Epesè: 0.5mm-30mm
3.Lajè: 1000-2000mm
4.Length: 1000-6000mm
ASTM A240 UNS S31700 plakse yon molybdène ki gen ba kabòn austenitic Nerjaveèi ak plis chromium, nikèl ak molybdène te ajoute pou pi bon rezistans nan korozyon ak atak chimik pa asid. Fèy Nerjaveèi asye 317L (UNS S31703) yo pa mayetik nan kondisyon an rkwit men yo ka yon ti kras mayetik apre soude. Konpozisyon chimik li yo ak pwopriyete fizik li yo fè li ideyal pou itilize nan petwochimik, jeni maren ak ekipman endistri chimik.
ASME SA240 UNS S31700 Plak Aplikasyon:
- Endistri pwosesis gaz
- Endistri petwochimik
- Endistri jenerasyon pouvwa
- Endistri Pwosesis Manje
- Endistri chimik yo
- Endistri lwil oliv ak gaz
- Endistri angrè
- Endistri sik

ASTM A240 SS 317 Espesifikasyon Plak
| Estanda | ASTM, ASME, BS, DIN, EN |
| Spesifikasyon | Fwad woule: 1219mm * 2438mm (4′ x 8′), 1219mm * 3048mm (4′ x 10′), 1220mm * 2440mm, 1250mm * 2500mm oswa kòm kondisyon ou. Cho woule: 1500mm * 2000mm, 1000mm * 3000mm, 1500mm * 4000mm, 1500m * 6000mm oswa kòm kondisyon ou. |
| Teknik | Plak woule cho (HR), fèy woule frèt (CR), 2B, 2D, BA NO (8), SATIN (Met ak plastik kouvwi) |
| Fòm | Fèy Shim, Fèy Perforé, Plak karo, retire rad sou ou, plat, elatriye. |
| Sifas | 2B, 2D, BA, NON. 1, NON. 4, NO.8, 8K, glas, karo, relief, liy cheve, sab eksplozyon, bwòs, grave |
| Epesè | {{0}}.25-200mm, 0.3mm rive 120mm |
| Lajè | 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm |
| Longè | 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, 12000mm |
| Pake | Pake Estanda Ekspòtasyon Seaworthy, oswa jan sa nesesè. |
| Sèvis Valè Te ajoute | Cladding, tretman chalè, rkwit, marinated, polonè, woule, koupe, koube, fòje, fabrikasyon minè elatriye. |
| MTC | Sètifika Tès Mill, Disponib dapre EN 10204 3.1 |
ASTM A240 TP317 Nerjaveèi asye plak pwopriyete fizik
| Pwopriyete | Metrik | Imperial |
|---|---|---|
| Dansite | 8 g/cm3 | 0.289 lb/pous³ |
| Pwen k ap fonn | 1370 degre | 2550 degre F |
ASTM A240 Nerjaveèi asye 317 Plak Pwopriyete mekanik
| Klas | SS 317 | |
| Fòs rupture (MPa) min | 515 | |
| Elongasyon (% nan 50mm) min | 35 | |
| Sede Fòs 0.2% Prèv (MPa) min | 205 | |
| Dite | Rockwell B (HR B) max | 95 |
| Brinell (HB) max | 217 | |
SS 317 Tablo pwa plak woule cho
|
Gwosè (mm) |
Pwa pou chak plak (Kg) |
Gwosè (mm) |
Pwa pou chak plak (Kg) |
|---|---|---|---|
|
4000 x 2000 x 2.0 |
136.0 |
3000 x 1500 x 5.0 |
191.0 |
|
4000 x 2000 x 3.0 |
204.0 |
4000 x 2000 x 5.0 |
340.0 |
|
2500 x 1250 x 4.0 |
106.0 |
2500 x 1250 x 6.0 |
159.0 |
|
3000 x 1500 x 4.0 |
153.0 |
3000 x 1500 x 6.0 |
230.0 |
|
4000 x 2000 x 4.0 |
272.0 |
4000 x 2000 x 6.0 |
408.0 |
|
2500 x 1250 x 5.0 |
133.0 |
- | - |
Estanda
- ASTM A240: Spesifikasyon estanda ki kouvri plak asye pur ak chalè ki reziste, fèy, ak teren.
- ASME SA-240: Estanda devlope pa Sosyete Ameriken an Enjenyè Mekanik (ASME) pou asye pur ak asye ki reziste chalè yo itilize nan chodyèr ak veso presyon.
FAQ
K: Ki sa ki pri Alloy 317 la?
K: Èske li nan stock?
K: Èske gen sèvis echantiyon?
K: Ki kantite minimòm lòd?
K: Konbyen tan se tan livrezon an?
K: Ki metòd peman yo sipòte?
K: Èske ou bay sètifika tès faktori?
K: Èske ou sipòte pwodwi Customized?
Baj popilè: astm a240 uns s31700 plak, astm a240 uns s31700, astm a240 31700, uns s31700
Ou ka renmen tou
Voye rechèch