HT PIPE se yon machann dirijan ak ekspòtatè mondyal ki gen plis pase 16 ane ekspètiz nan komès entènasyonal. Nou bay tiyo, plak, ba wonn, ak yon seri konplè nan ekipman tiyo, bride, ak tiyo.Kontakte noukounye a pou site gratis ak enfòmasyon sou pwodwi pèsonalize.
Konpare Valè: 316L vs . 316 Diferans Pri Tiyo
Yon kesyon souvan pandan faz konsepsyon pwojè yo se si w chwazi Klas 316L chanje ekonomi pwojè yo konpare ak Klas 316 estanda.
Soti nan yon pèspektiv matyè premyè, delta pri baz ant 316 ak 316L se majinal (souvan mwens pase yon diferans 2-3%). Sepandan, retounen sou envestisman (ROI) 316L bay se sibstansyèl:
Eliminasyon Tretman Chalè Post-soude (PWHT):Piske 316L evite presipitasyon carbure chromium pandan soude, ou ekonomize anpil travay sou plas -kout travay ak pwosesis.
Alontèm -Viv sèvis:Rezistans amelyore nan pike ak kowozyon nan fant nan klori-anviwònman ki rich yo anpeche krak korozyon estrès twò bonè, minimize fèmen antretyen ki pa pwograme.
Pri nan SS 316/316L lis pri tiyo san pwoblèm
| Pwodwi | Pri nan ($) |
| • SS 316 tiyo san pwoblèm ASTM A312 TP 316 | $ 5400 ~ $ 6900 USD/Tòn |
| • SS 316L san pwoblèm tiyo ASTM A312 TP 316L | $ 5500 ~ $ 7000 USD/Tòn |
| • SS 316 ERW/soude tiyo ASTM A312 TP 316 | $ 4900 ~ $ 6400 USD/Tòn |
| • SS 316L ERW/soude tiyo ASTM A312 TP 316L | $ 5000 ~ $ 6500 USD/Tòn |
| • SS 316 EFW tiyo ASTM A358 TP 316 | $ 4500 ~ $ 6000 USD/Tòn |
| • SS 316L EFW tiyo ASTM A358 TP 316L | $ 4700 ~ $ 6200 USD/Tòn |
Pri Nerjaveèi 316/316L Tib
| Pwodwi | Pri nan ($) |
| • SS 316 Tib san pwoblèm/Tub ASTM A269 TP 316 | $ 6400 ~ $ 7900 USD/Tòn |
| • SS 316L Tib san pwoblèm/Tub ASTM A269 TP 316L | $ 6500 ~ $ 8000 USD/Tòn |
| • SS 316 ERW/soude Tib/Tub ASTM A249 TP 316 | $ 5900 ~ $ 7400 USD/Tòn |
| • SS 316L ERW/soude Tib/Tub ASTM A249 TP 316L | $ 6000 ~ $ 7500 USD/Tòn |
| • SS 316 Tib echanjeur chalè/tib ASTM A213 TP 316 | $ 6400 ~ $ 7900 USD/Tòn |
| • SS 316L Tib echanjeur chalè/tib ASTM A213 TP 316L | $ 6400 ~ $ 7900 USD/Tòn |
| • SS 316 Transparans Bright Anealed Tib/Tub ASTM A269 TP 316 | $ 6400 ~ $ 7900 USD/Tòn |
| • SS 316L Transparans Bright Anealed Tib/Tub ASTM A269 TP 316L | $ 6400 ~ $ 7900 USD/Tòn |
316/316L Nerjaveèi tiyo Dimansyon & Pousantaj
| Nominal Bore | Dyamèt deyò | Sch-5S | Pousantaj (Pri) | Sch-10S | Pousantaj (Pri) | Sch-40S | Pousantaj (Pri) | ||||
| mm | POUS | mm | Pwa mm | Pwa (Kg/mt) | Pwa mm | Pwa (Kg/mt) | Rs/Kg | Pwa mm | Pwa (Kg/mt) | Rs/Kg | |
| 3 | 1/8 | 10.3 | 1.24 | 0.276 | 288.90 | 1.24 | 0.28 | 321.00 | 1.73 | 0.37 | 343.47 |
| 6 | 1/4 | 13.7 | 1.24 | 0.390 | 288.90 | 1.65 | 0.49 | 321.00 | 2.24 | 0.631 | 343.47 |
| 10 | 3/8 | 17.1 | 1.24 | 0.490 | 278.20 | 1.65 | 0.63 | 267.50 | 2.31 | 0.845 | 286.23 |
| 15 | 1/2 | 21.3 | 1.65 | 0.800 | 262.15 | 2.11 | 1.00 | 283.55 | 2.77 | 1.27 | 303.40 |
| 20 | 3/4 | 26.7 | 1.65 | 1.03 | 256.80 | 2.11 | 1.28 | 278.20 | 2.87 | 1.68 | 297.67 |
| 25 | 1 | 33.4 | 1.65 | 1.30 | 256.80 | 2.77 | 2.09 | 278.20 | 3.38 | 2.50 | 297.67 |
| 32 | 1 1/4 | 42.2 | 1.65 | 1.65 | 267.50 | 2.77 | 2.70 | 278.20 | 3.56 | 3.38 | 297.67 |
| 40 | 1 1/2 | 48.3 | 1.65 | 1.91 | 267.50 | 2.77 | 3.11 | 278.20 | 3.68 | 4.05 | 297.67 |
| 50 | 2 | 60.3 | 1.65 | 2.40 | 267.50 | 2.77 | 3.93 | 278.20 | 3.91 | 5.44 | 297.67 |
| 65 | 2 1/2 | 73.0 | 2.11 | 3.69 | 267.50 | 3.05 | 5.26 | 278.20 | 5.16 | 8.63 | 297.67 |
| 80 | 3 | 88.9 | 2.11 | 4.51 | 267.50 | 3.05 | 6.45 | 278.20 | 5.49 | 11.30 | 297.67 |
| 100 | 4 | 114.3 | 2.11 | 5.84 | 267.50 | 3.05 | 8.36 | 278.20 | 6.02 | 16.07 | 297.67 |
| 125 | 5 | 141.3 | 2.77 | 9.47 | 278.20 | 3.40 | 11.57 | 283.55 | 6.55 | 21.8 | 303.40 |
| 150 | 6 | 168.3 | 2.77 | 11.32 | 278.20 | 3.40 | 13.84 | 283.55 | 7.11 | 28.3 | 303.40 |
| 200 | 8 | 219.1 | 2.77 | 14.79 | 288.90 | 3.76 | 19.96 | 288.90 | 8.18 | 42.6 | 309.12 |
| 250 | 10 | 273.1 | 3.40 | 22.63 | 294.25 | 4.19 | 27.78 | 299.60 | 9.27 | 60.5 | 320.57 |
| 300 | 12 | 323.9 | 3.96 | 31.25 | 299.60 | 4.57 | 36.00 | 299.60 | 9.52 | 73.88 | 320.57 |
| 350 | 14 | 355.6 | 3.96 | 34.36 | 4.78 | 41.3 | 299.60 | 11.13 | 94.59 | 320.6 | |
| 400 | 16 | 406.4 | 4.19 | 41.56 | 4.78 | 47.29 | 299.60 | 12.7 | 123.30 | 320.57 | |
| 450 | 18 | 457.2 | 4.19 | 46.80 | 4.78 | 53.42 | 299.60 | 14.27 | 155.80 | 320.57 | |
| 500 | 20 | 508.0 | 4.78 | 59.25 | 5.54 | 68.71 | 299.60 | 15.09 | 183.42 | 320.57 | |
| 600 | 24 | 609.6 | 5.54 | 82.47 | 6.35 | 94.45 | 299.60 | 17.48 | 255.41 | 320.57 | |
Yon entwodiksyon tou kout sou SS 316L tiyo san pwoblèm:
Alyaj 316l|UNS S31603|1.4404|1.4435se yon materyèl tiyo ki trè reziste -kowozyon nan lavni ki souvan itilize nan aplikasyon endistriyèl ak chimik ki mande pou yon wo degre de rezistans korozyon. Men kèk karakteristik kle ak benefis yo:
- 316L materyèl asye pur:Nerjaveèi asye 316L tiyo san pwoblèm, ki se yon ba-kabòn Nerjaveèi ak pi bon rezistans korozyon epi li espesyalman apwopriye pou anviwònman ki gen gwo kondisyon rezistans korozyon.
- Manifakti tiyo san pwoblèm: Konpare ak tiyo soude,ss 316l tiyo san pwoblèmgen yon estrikti plis inifòm ak pi wo rezistans presyon. Pwosesis fabrikasyon tiyo san pwoblèm enplike chofaj ak pèfore tiyo yo pou kreye tiyo san pwoblèm.
- Rezistans korozyon:Tiyo alyaj 316L asye purse li te ye pou rezistans ekselan korozyon li yo epi li se patikilyèman apwopriye pou aplikasyon k ap travay nan anviwònman asid oswa alkalin. Kalite tiyo sa a trè rezistan a anpil pwodui chimik.
- Pèfòmans tanperati ki wo:Tib AISI 316Lka toujou kenbe fòs yo ak rezistans korozyon nan anviwònman tanperati ki wo, fè yo apwopriye pou pwosesis endistriyèl ki mande estabilite tanperati ki wo.
- Lajman itilize: Sa a kaliteSCH 40 316L asye pur tiyo san pwoblèmse lajman ki itilize nan petrochimik, pharmaceutique, pwosesis manje, endistri konstriksyon bato ak lòt jaden, kote gen gwo kondisyon pou rezistans korozyon ak pite materyèl.