Nerjaveèi asye s316l vs super duplex asye pur 2507

316L asye pur ak Super asye pur 2507 founisè manifakti. Kontakte nou jwenn gratis quote ak echantiyon!

 

Austenitik asye pur S316L (UNS S31603)akSuper Duplex Nerjaveèi asye 2507 (UNS S32750)Gen diferans siyifikatif nan konpozisyon chimik, karakteristik pèfòmans ak jaden ki aplikab yo. S316L has become a common choice in petrochemical, food processing and other fields due to its good corrosion resistance and processing performance. 2507 duplex steel, with its dual-phase microstructure and ultra-high alloy content, shows irreplaceable value in harsh environments, especially in high-temperature and high-pressure environments containing chloride ions.

 

Nerjaveèi asye S316L ak S32750 Microstructure

S316L: prezante yon sèl-faz estrikti austenitik (figi ki santre estrikti kib), ki bay li ekselan severite ak formability, men se tendans estrès korozyon fann (SCC) anba estrès segondè oswa klori ki gen anviwònman.

 

2507: Atravè tretman chalè egzak (rapid refwadisman nan 1000-1050 degre), yon estrikti duplex ak austenit + ferit kontablite pou apeprè 50% chak jwenn. Estrikti sa a konbine fòs la nan ferit ak severite nan austenit, pandan y ap adisyon a nan nitwojèn siyifikativman amelyore rezistans korozyon. Fwontyè a grenn jaden ant de faz yo kapab tou efektivman anpeche pwopagasyon krak, bay materyèl la ekselan estrès rezistans korozyon.

 

316l

2507 Steel ak SS316L Pèfòmans nan anviwònman klori

Pitting ak fant korozyon:Nan anviwònman ion klori (tankou dlo lanmè ak espre sèl), fim nan pasivasyon nan S316L se fasil lokalman kraze, sa ki lakòz kowozyon nan panno. S31803, sepandan, te siyifikativman amelyore rezistans pitting li yo akòz gwo valè pre li yo (pi gran pase oswa egal a 42.5). Tès ASTM G48 montre ke tanperati a kritik opozisyon (CPT) nan 2507 nan 6% solisyon FECL₃ se kòm yon wo 70 degre oswa plis, pi wo pase apeprè 25 degre nan S316L.

 

Estrès korozyon fann (SCC):Austenitic stainless steel is prone to SCC in chloride environments >60 degre. Estrikti a doub-faz nan 2507 anpil amelyore rezistans SCC li yo pa bloke chemen an pwopagasyon krak nan faz la ferit, ak prèske pa gen okenn fann rive nan anviwònman an menm.

 

S31603 ak S32750 Diferans nan repons korozyon nan medya asid

Anviwònman asid silfirik:Nan asid silfirik dilye (<20%), 2507 outperforms S316L due to its high chromium and molybdenum content; in concentrated sulfuric acid (>90%) anviwònman, 904L austenitik asye pur se pi apwopriye.

 

Aplikasyon asid òganik:S32750 gen ekselan rezistans nan asid òganik tankou asid fòmik ak asid acetic, epi li se apwopriye pou ekipman pwodiksyon asid acetic. Malgre ke S316L ka satisfè bezwen debaz nan anviwònman sa yo, li ka fè fas a defi anba tanperati ki wo ak kondisyon konsantrasyon segondè.

 

Limit asid idroklorik:S316L entèdi pou yo te itilize nan anviwònman asid idroklorik, e menm konsantrasyon ki ba ka fasilman lakòz korozyon konplè, pandan y ap 2507 ka itilize nan asid idroklorik dilye (<5%), but the concentration and temperature parameters need to be carefully evaluated. 

 

Kle konpozisyon chimik konparezon

Eleman S316L 2507
Cr 16-18% 24-26%
NI 10-12% 6-8%
Mwa 2-3% 3-5%
N Mwens pase oswa egal a 0.10% 0.24-0.32%
C Mwens pase oswa egal a 0.03% Mwens pase oswa egal a 0.03%
Pre ~25 Pi gran pase oswa egal a 42.5

 

Kle Fizik & Pwopriyete mekanik Konparezon

Posesyon S316L 2507
Sede fòs Pi gran pase oswa egal a 170 MPa Pi gran pase oswa egal a 550 MPa
Ekspansyon tèmik 16.5 μm/m degre 13.0 μm/m degre
Tèmik konduktivite 13 w/mk 15 w/mk
Dansite 8.0 g/cm³ 8.03 g/cm³
Modil elastik 193 GPA 200 GPA

 

Jaden ekonomik ak aplikab nan S316L

  • Biopharmaceutique ak manje tuyaux:satisfè estanda ijyèn, tolere ajan netwayaj asid òganik, epi yo lajman itilize nan tank fèmantasyon ak tuyaux dlo pi
  • Anviwònman chimik modere:Nan sistèm asid ki gen kontni ion klori ki ba (<200 ppm) and moderate temperature, such as dye intermediate production equipment
  • Bati rezèv dlo ak sistèm drenaj:Urban tiyo dlo tretman tiyo plant, kote konsantrasyon an ion klori se kontwole epi pa gen okenn tanperati ki wo ak presyon ki wo

 

Senaryo iranplasabl pou 2507

  • Offshore lwil oliv ak gaz platfòm:high PRE value (≥42.5) meets the requirements of PRE>40 pou sistèm piki dlo lanmè.
  • Lanmè dlo desalination gwo presyon tiyo:Nan seksyon an presyon-wo (5.5-7 MPa) apre osmoz la ranvèse (RO) manbràn, 2507 gen tou de anti-cl⁻ korozyon ak karakteristik fòs segondè, ak lavi sèvis li yo ka rive jwenn plis pase 3 fwa sa yo ki an 316L.
  • Sistèm desulfurizasyon gaz fwit chemine:Tiyo a sikilasyon gwo kay won absòpsyon bezwen tolere CL⁻ konsantrasyon, SO₂ anviwònman asid ak sann abrazif an menm tan an. Pèfòmans konplè nan 2507 se pi bon pase 316L isit la.

 

316L asye pur ak Super asye pur 2507 founisè manifakti

Avèk 15 ane nan ekselans ekspòtasyon, HT tiyo se stockist serye ou ak ekspòtatè. Pòtfolyo nou an gen ladanASTM A269 Tp316L tiyo, ASTM A240 UNS S32750 Plak, ba wonn, ak yon etalaj lajè nan ekipman, èl, ak Pwodwi pou Telefòn soude. Kontakte nou jodi a pou prix pa gen okenn-obligasyon ak detay pwodwi-nou ap pare yo sipòte pwojè ou yo.