TUYO EN STEEL

Espesifikasyon tiyo ASTM Klas UNS ekivalan EN Ekivalan Ekivalan Werkstoff
ASTM A312 / 358 & EN 10216-2 San pwoblèm / EN 10217-5 Soude 304 S30400 X5CrNi18-10 1.4301
304L S30403 X2CrNi19-11 1.4306
304H S30409 X6CrNi18-11 1.4948
310 S31000 X15CrNiSi25-21 1.4841
310S S31008 X8CrNi25-21 1.4845
316 S31600 X5CrNiMo17-12-2 1.4401
316L S31603 X2CrNiMo17-2-2 1.4404
316Ti S31635 X6CrNiMoTi17-12-2 1.4571
321 S32100 X6CrNiTi18-10 1.4541
321H S32109 X8CrNiTi18-10 1.4878
347 S34700 X6CrNiNb18-10 1.455
347H S34709 X8CrNiNb16-13 1.4961
6Mo S31254 X1CrNiMoCuN25-20-7 1.4529
904L N08904 X1NiCrMoCu25-20-5 1.4539
ASTM A790 / A928 & EN 10216-2 San pwoblèm / EN 10217-5 Soude Duplex S31260 X2CrNiMoN25-7-4 1.441
Duplex S32900 X3CrNiMoN27-5-2 1.446
Duplex S31803 / S32205 X2CrNiMoN22-5-3 1.4462
Super duplex S32760 X2CrNiMoCuWN25-7-4 1.4501
Super duplex S32750 / S32550 X2CrNiMoCuN25-6-3 1.4507

 

TUYO ALOYY NIKÈL

Alyaj Espesifikasyon tiyo ASTM
(San pwoblèm)
Espesifikasyon tiyo ASTM
(soude)
UNS DIN ekivalan Ekivalan Werkstoff
Alyaj 20 B729 B464 N08020   2.466
Nikèl 200 B161 B622 N02200   2.4060/2.4066
Nikèl 201 B161 B622 N02201   2.4061/2.4068
Monel 400 B165 B725 N04400   2.436
Inconel 600 B167 B517 N06600   2.4816
Inconel 625 B444 B705 N06625   2.4856
Incoloy 800H/800HT B407 B514 N08811   1.4959
Incoloy 825 B423 N/A N08825   2.4858
Hastelloy C276 B622 B619 N10276   2.4819
  B619 B619 N10675 NiMo29Cr 2.46
  B622 B619 N06022 NiCr21Mo14W 2.4602
  B622 B619 N06455 NiMo16Cr16Ti 2.461
  B622 B619 N10276 NiMo16Cr15W 2.4819
  B622 B619 N06200 NiCr23Mo16Cu 2.4675
  B622 B619 N06030 NiCr30FeMo 2.4603
  B622 B619 N06035 NiCr33Mo8 2.4643
  B622 B619 N10362 NiMo22Cr15 2.4708

 

TUYO STEEL ALOYY

Aplikasyon Espesifikasyon tiyo Klas Materyèl
Tiyo asye alyaj (wo presyon/tanperati) ASTM/ASME A/SA 335 P1, P5, P9, P11, P22, P91, P92
ASTM/ASME A/SA 691 1-1/4CR, 2-1/4CR, 5CR, 9CR, 91
EN 10216-2 San pwoblèm 16Mo3 (1.5415)
13CrMo4-5 (1.7335)
10CrMo9-10 (1.7380)
11CrMo9-11 (1.7383)
X10CrMoVnb9-1 (1.4903)
X10CrWMoVnb9-2 (1.4901)
WB36 – 15NiCuMoNb5-6-4 (1.6368)
10CrMo5-5 (1.7338)14MoV6-3 (1.7715)
EN 10217-5 Soude 16Mo3 (1.5415)
13CrMo4-5 (1.7335)
10CrMo9-10 (1.7380)
11CrMo9-11 (1.7383)
X10CrMoVnb9-1 (1.4903)
X10CrWMoVnb9-2 (1.4901)
WB36 – 15NiCuMoNb5-6-4 (1.6368)
10CrMo5-5 (1.7338)14MoV6-3 (1.7715)

 

TIYO STEEL KABÒN

Aplikasyon Espesifikasyon tiyo Klas Materyèl
High-tanperati Kabòn Steel EN 10225 S355G15, S460G6
BS 7191 355EM
API 5L Klas B, X42, X52, X56, X60, X65, X70, X80, X100
ASTM A519 SAE 4130, 4140
ASTM/ASME A/SA53 Klas A, B
ASTM A252 Klas 2, 3
Liy tiyo CSA Z245.1 359, 414, 448, 483
ASTM/ASME A/SA53 Klas A, B
ASTM/ASME A/SA106 Klas B, C
ASTM A252 Klas 2, 3
EN 10216-2 San pwoblèm P235GH (1.0345) / P265 GH (1.0425)
EN 10217-5 Soude P235GH (1.0345) / P265GH (1.0425)
Tanperati ki ba ASTM/ASME A/SA333 P215NL (1.0451)
EN 10216-3  
P355N (1.0562)
P355NH (1.0565)
P355NL1 (1.0566)
P275NL1 (1.0488)
P275NL2 (1.1104)
L290NB (1.0484)
L360NB (1.0582)
ASTM/ASME A/SA 671/672 Klas 60, 65, 70

 

 