ASTM B729 UNS N08020 Tib|Alloy 20 tiyo san pwoblèm

ASTM B729 UNS N08020oswachapant 20Kontni nikèl diferan de nivo asye pur konvansyonèl yo.Alloy 20 tiyo san pwoblèmgen kwiv epi li gen gwo tolerans pou asid silfirik. Anplis de silfat, lè klori oswa asid (asid nitrique ak fosfat). Anplis de sa, chak echantiyon oswa eleman ki fè pati nanASTM B729 UNS N08020 tiyote teste pa tès dlo estatik oswa tès elektrisite ki pa destriktif. AlLoy 20 ka itilize pou echanjeur chalè, pwodui chimik ak ekipman pwosesis petwòl.

 

ASTM B729 UNS N08020 Tiyo Chimik Konpozisyon

Alyaj 20 Ni C Mo Mn Si Fe Cu S P Kr
32 – 38 0.02 max 2 – 3 1 – 2 0.7 max Bal 3 – 4 0.005 max 0.02 max 19 – 21

 

20cb3 Carpenter 20 Tib san pwoblèm pwopriyete mekanik

Dansite Pwen k ap fonn Fòs Sede (0.2% Offset) Fòs rupture Elongasyon
8.1 g/cm3 1443 degre (2430 degre F) Psi - 35000, MPa - 241 Psi - 80000, MPa - 551 30 %

 

2.4660 Alloy 20 Tubing Espesifikasyon ekivalan

ALLOY UNS WERKSTOFF NR. AFNOR EN JIS BS GOST
Alyaj 20 N08020 2.4660 Z2NCUD31-20AZ NiCr20CuMo – – –

 

ASTM B729-20 Estanda

  • Espesifikasyon estanda pou tiyo ak tib alyaj nikèl san pwoblèm nikèl-fè-kwòm-molybdène-kwiv
  • ASTM B729spesifikasyon kouvri UNS N08020, UNS N08026 ak UNS N08024 nikèl-alyaj san pwoblèm, frèt-travay oswa cho-fini tiyo ak tib gen entansyon pou sèvis jeneral korozivite.

 

Founisè alyaj 20 tiyo

HT PIPE se yon founisè ak manifakti tib Alloy 20 la.Kontakte noupou jwenn plis enfòmasyon ak sitasyon pi ba gratis!

 

Nou ka bay tiyo san pwoblèm ak soude.Alyaj 20 tiyo san pwoblèmgen yon seri dyamèt deyò de {{0}}.375 pous a 1 pous, ak tiyo soude varye ant 0.125 pous ak 1 pous. Tiyo san pwoblèm gen pi wo presyon pote kapasite ak fòs pase tiyo soude. Epesè miray ak pwa tou gen yon bagay fè ak tiyo san pwoblèm ak soude.

 

 

Voye rechèch

whatsapp

Telefòn

Mel

Rechèch