ASTM B163 Tib Pwopriyete mekanik
ASTM B163se yon spesifikasyon estanda pou nikèl san pwoblèm ak nikèl alyaj kondansateur ak tib echanjeur chalè. Tib yo fèt espesyalman pou kenbe tèt ak tanperati ki wo ak presyon pandan y ap bay ekselan rezistans korozyon. Pwopriyete sa yo fè yo ideyal pou itilize nan divès aplikasyon endistriyèl, ki gen ladan pwosesis chimik ak petrochimik, jenerasyon pouvwa, ak desalinasyon dlo lanmè.
Konpayi nou an se yon founisè ASTM B163 Tib ak plis pase 15 ane eksperyans nan ekspòtasyon. Nou ka bayASTM B163 UNS N02200 Tib, ak N02201, N06601, N04400, N06600, elatriye Tanpri kontakte nou pou plis enfòmasyon ak quotes gratis!
Pwopriyete mekanik nan tib ASTM B163
| Materyèl | Kondisyon | Fòs rupture min ksi (MPa) |
Fòs Sede (0.2 % Offset) min psi (MPa) |
Elongasyon nan 2 pous oswa 50 mm (oswa 4 D) min% | Rockwell Hardness (oswa ekivalan) pou bout rkwitA |
| Ni UNS N02200 |
Rkwit | 55(379) | 15(103) | 40 | ... |
| Estrès-soulaje | 65(448) | 40(276) | 15 | Mwens pase oswa egal a B65 | |
| Ba-kabòn Ni UNS N02201 |
Rkwit | 50(345) | 12(83) | 40 | ... |
| Estrès-soulaje | 60(414) | 30(207) | 15 | Mwens pase oswa egal a B62 | |
| Ni-Cur alyaj UNS N04400 |
Rkwit | 70(483) | 28(193) | 35 | ... |
| Estrès-soulaje | 85(586) | 55(379) | 15 | Mwens pase oswa egal a B75 | |
| Ni-Cr-Fer alyaj | Recuit alyaj UNS N06600 | 80(552) | 35(241) | 30 | … |
| Alyaj rkwit UNS N06601 | 80(552) | 30(207) | 30 | … | |
| Alyaj rkwit UNS N06690 | 85(586) | 35(241) | 30 | … | |
| Alyaj rkwit UNS N06045 | 90(620) | 35(240) | 35 | … | |
| Alyaj rkwit UNS N06025 | 98(680) | 39(270) | 30 | … | |
| Alyaj rkwit UNS N06603 | 94(650) | 43(300) | 25 | … | |
| Ba-kabòn Ni-Cr-Mo-Wr alyaj | Rekwit UNS N06686 | 100(690) | 45(310) | 45 | … |
| Ni-Fe-Crr alyaj | Recuit alyaj UNS N08120 | 90(620) | 40(276) | 30 | … |
| Recuit alyaj UNS N08800 | 75(517) | 30(207) | 30 | … | |
| Alyaj rkwit UNS N08801 | 65(448) | 25(172) | 30 | … | |
| Fwad-travay UNS N08800 | 83(572) | 47(324) | 30 | … | |
| Alyaj rkwit UNS N08810 | 65(448) | 25(172) | 30 | … | |
| Alyaj rkwit UNS N08811 | 65(448) | 25(172) | 30 | … | |
| Ni-Fe-Cr-Mo-Cur alyaj | Rekwit UNS N08825 | 85(586) | 35(241) | 30 | … |
ARockwell oswa valè dite ekivalan aplike sèlman nan pwent rkwit tib ki soulaje estrès yo. Yo ta dwe obsève atansyon lè w ap itilize tès Rockwell la sou materyèl mens, paske rezilta yo ka afekte pa epesè echantiyon an. Pou epesè anba 0.050 pous (1.27 mm) yo sijere itilize Rockwell sipèfisyèl oswa tès dite Vickers la. Pou konvèsyon dite pou nikèl ak alyaj ki gen anpil nikèl, gade Tablo Konvèsyon Dite E 140.
Pwopriyete mekanik ASTM B163 Ti Dyamèt ak Tib Mi limyè
| Materyèl | Fòs rupture ksi (MPa) |
Fòs Sede (0.2 % konpanse)B min ksi (MPa) |
Elongasyon nan 2 pous oswa 50 mm min % | Rockwell diteC (Echèl jan sa endike) |
|
| Ni UNS N02200 |
RkwitD | Mwens pase oswa egal a 80(552) | 15(103) | 33 | Mwens pase oswa egal a B75 |
| Mwatye-difisilE | Pi gran pase oswa egal a 80(552) | 40(276) | 12 | B75-B90 | |
| Full difisilF | Pi gran pase oswa egal a 95(655) | 75(517) | 4 | B90-C30 | |
| Ba-kabòn Ni UNS N02200 |
RkwitD | Mwens pase oswa egal a 70 (483) | 12(83) | 35 | Mwens pase oswa egal a B62 |
| Mwatye-difisilE | Pi gran pase oswa egal a 70(483) | 30(207) | 12 | B70-B85 | |
| Full difisilF | Pi gran pase oswa egal a 85(586) | 65(448) | 4 | B80-B95 | |
| Ni-Cu alyaj UNS N04400 |
RkwitD | Mwens pase oswa egal a 90 (621) | 28(193) | 32 | Mwens pase oswa egal a B80 |
| Mwatye-difisilE | Pi gran pase oswa egal a 85(586) | 55(379) | 12 | B75-B97 | |
| Full difisilF | Pi gran pase oswa egal a 110(758) | 90(621) | 3 | B95-C27 | |
| Ni-Cr-Fe alyaj UNS N06600 |
RkwitKAYE | 80(552)-110(758) | 35(241) | 30 | Mwens pase oswa egal a B92 |
| Mwatye-difisilE | Pi gran pase oswa egal a 105(724) | 55(379) | 13 | B90-B98 | |
| Full difisilF | Pi gran pase oswa egal a 130(896) | 105(724) | 4 | C19-C34 | |
| Ni-Cr-Fe alyaj UNS N06601 |
RkwitKAYE | 80(552)-110(758) | 35(241) | 30 | Mwens pase oswa egal a B92 |
| Mwatye-difisilE | Pi gran pase oswa egal a 105(724) | 55(379) | 13 | B90-B98 | |
| Full difisilF | Pi gran pase oswa egal a 130(896) | 105(724) | 4 | C19-C34 | |
| Ni-Cr-Fe alyaj UNS N06690 |
RkwitKAYE | 85(586)-115(793) | 35(241) | 30 | Mwens pase oswa egal a B92 |
| Mwatye-difisilE | Pi gran pase oswa egal a 105(724) | 55(379) | 13 | B90-B98 | |
| Full difisilF | Pi gran pase oswa egal a 130(896) | 105(724) | 4 | C19-C34 | |
| Ni-Fe-Cr alyaj UNS N08800 |
RkwitDG | 75(517)-100(689) | 30(207) | 30 | Mwens pase oswa egal a B95 |
| Mwatye-difisilE | 105(724) | 60(414) | 13 | B93-C26 | |
| Full difisilF | 130(896) | 105(724) | 4 | C24-C38 | |
| Ni-Fe-Cr-Mo-Cu alyaj UNS N08825 |
RkwitKAYE | 85(586)-115(793) | 35(241) | 30 | Mwens pase oswa egal a B90 |
| Mwatye-difisilE | Pi gran pase oswa egal a 105(724) | 75(517) | 15 | B90-C25 | |
| Full difisilF | Pi gran pase oswa egal a 125(862) | 100(689) | 5 | C25-C35 | |
APa aplikab pou dyamèt deyò anba 1⁄8 pous (3.2 mm) ak pou epesè miray anba 0.015 pous (0.38 mm).
BGade 12.3.
CValè dite, ki endike fòs rupture, yo montre pou enfòmasyon sèlman. Tout tès yo sijè a konfimasyon pa tès tansyon. Pou konvèsyon dite, gade Tablo konvèsyon dite E 140.
DKondisyon sa a pafwa deziyen kòm "No 1 Tanperaman."
EKondisyon sa a pafwa deziyen kòm "No 2 Tanperaman."
FKondisyon sa a pafwa deziyen kòm "No 3 Tanperaman."
GValè minimòm fòs rupture aplike sèlman nan tib nan longè dwat.