254 SMO (UNS S31254, 6MO, EN 1.4547) is a corrosion resistant austenitic stainless steel. It has a Pitting Resistance Equivalent Number (PREN) of 43-46. 6MO material performs exceptionally well in environments with high chloride concentrations (>3000 ppm Cl⁻), fè li rezistan a korozyon dlo lanmè. Li gen tou siperyè estrès korozyon krak (SCC) rezistans konpare ak 316L ak 904L asye pur.

 

254smo Nerjaveèi asye Fòm ki disponib

Nou se yon Pwofesyonèl One-Stop Sèvis Fabricants Founisè Ekspòtè

SS 1.4547 Material

Kontakte kounye a

 

EN 1.4547 Konpozisyon chimik asye (valè tipik, %)

Eleman Konpozisyon (%)
Kabòn (C) Mwens pase oswa egal a 0.02
Manganèz (Mn) Mwens pase oswa egal a 1.00
Fosfò (P) Mwens pase oswa egal a 0.030
Souf (S) Mwens pase oswa egal a 0.010
Silisyòm (Si) Mwens pase oswa egal a 0.80
Kwòm (Cr) 19.5 - 20.5
Nikèl (Ni) 17.5 - 18.5
Molybdène (Mo) 6.0 - 6.5
Kwiv (Cu) 0.5 - 1.0
Azòt (N) 0.18 - 0.22

 

Pwopriyete mekanik UNS S31254 6MO (valè tipik nan tanperati chanm)

Pwopriyete Valè
Fòs rupture (MPa) Pi gran pase oswa egal a 950
Fòs Sede (0.2% Offset) (MPa) ≩440
elongasyon (%) Pi gran pase oswa egal a 35
Dite (Brinell) Mwens pase oswa egal a 280
Severite enpak (J) >100

 

254 SMO UNS S31254 Tretman Chalè

254 SMO se solisyon annealed ant 1150-1200 degre ki te swiv pa refwadisman rapid.

 

Alloy 254 SMO soude ak fabrikasyon

  • Metòd soude: GTAW (TIG), GMAW (MIG) ak SMAW (baton) soude.
  • Materyèl filler: Filler filler rekòmande yo enkli AWS A5.9 ERNiCrMo-3 oswa ERNiCrMo-10.
  • Machinability: Zouti byen file ak manje dousman obligatwa pou pi bon rezilta.

 

S31254 Steel Aplikasyon

  • Marin ak Offshore: tiyo dlo lanmè, echanjeur chalè, plant desalination.
  • Pwosesis chimik: ekipman manyen asid, réacteurs ak tank depo.
  • Endistri kaka ak papye: sistèm klowòks dyoksid klò.
  • Pwosesis manje: anviwònman salinite segondè, etan sèl.

 

Sekirize materyèl segondè -alyaj ou yo nan HT PIPE

HT PIPE bay gwo -pèfòmans, konplètman sètifye6MO S31254 pwodwi asye purakonpaye pa konplè EN 10204 3.1 Sètifika Tès Mill. Soti nan gwo -echèl bobin tiyo endistriyèl rive nan dimansyon plak matyè premyè yo vit-, rezo lojistik nou an bay livrezon entènasyonal ki an sekirite.

 

Kontakte Ekip Komèsyal Jeni nou anjodi a pou resevwa yon sitasyon materyèl konpetitif, verifye pwa stock aktyèl yo, oswa mande fich teknik.

 

Voye rechèch

whatsapp

Telefòn

Mel

Rechèch