| Klas | C | Mn | sizo | P | S | Kr | Nb + Ta | Kolòn | Mouvman | Fe | al | Tibèkil | Ni |
| 625 | Mwens pase oswa egal a 0.100 | Mwens pase oswa egal a 0.500 | Mwens pase oswa egal a 0.500 | Mwens pase oswa egal a 0.015 | Mwens pase oswa egal a 0.015 | 20.000 - 23.000 | 3.150 -4.150 | Mwens pase oswa egal a 1.000 | 8.000-10.000 | Mwens pase oswa egal a 5.000 | Mwens pase oswa egal a 0.400 | Mwens pase oswa egal a 0.400 | Bal |

Inconel 625 tiyo san pwoblèm
1. estanda: ASTM B444, ASME SB444, ASTM B474, ASME SB474
2. OD: 1/2" - 4"
3. epesè miray la: SCH10 - SCH160
4. Longè: Single o aza, doub o aza, oswa koupe longè
Inconel 625 tiyo san pwoblèmse yon alyaj nikèl-chromium ak ekselan rezistans nan korozyon ak oksidasyon tanperati ki wo. ASTM B444 UNS N06625 tiyo san pwoblèm gen yon fòs sede minimòm de 517MPa ak yon fòs rupture minimòm de 930MPa. Tanperati a maksimòm opere nan Inconel 625 alyaj se 980 degre ak pwen an k ap fonn se 1350 degre. Alloy 625 tiyo san pwoblèm tou gen bon soudabilite epi yo ka fasilman fòme nan yon varyete de fòm. Kontakte nou |market@htpipe.compou plis enfòmasyon ak yon quote gratis!
Inconel 625 san pwoblèm soude tiyo estanda ASTM:
- ASTM B444: Spesifikasyon pou alyaj nikèl-kwòm-molybdène-kolonbyòm (UNS N06625 ak UNS N06852) ak alyaj nikèl-kwòm-molybdène-silikon (UNS N06219) tiyo ak tib
- ASTM B474: Spesifikasyon estanda pou fizyon elektrik soude nikèl ak tiyo alyaj nikèl
- Founisè: Nou ofri tou fil Inconel 625, ba, fèy / plak, tib, ekipman, bride, forgings, ak baton soude.

Inconel 625 Espesifikasyon tiyo san pwoblèm
| Estanda | ASTM, ASME, JIS%, AISI, AMS, EN, SAE, DIN, NF, TOCT, DS, DTD, GB |
| Gwosè tiyo san pwoblèm | 4 a 219mm WT: 0.5 a 20mm |
| Orè | XS, SCH30, SCH40, XXS, SCH80, SCH120, SCH60, SCH140, STD, SCH10, SCH10S, SCH40S, SCH80, SCH20, SCH5, SCH160 |
| Longè | Double Random, Single Random, Standard & Koupe longè tiyo |
| Fini | Poli, AP (Annealed & marinated), BA (Klere & Recuit), MF, NO.1, NO.4, 2B, BA, HL, 8K, Miwa fini, elatriye |
| Kalite | San pwoblèm |
| Fen tiyo | Plain Fen, Bizote Fen, Treaded Tiyo, Vise pwent |
| Aplikasyon | Tiyo letye, tiyo lwil oliv, tiyo gaz, tiyo likid, tiyo chodyè pou endistri chimik |
| Sèvis Valè Te ajoute | Trase & ekspansyon jan pou chak egzije gwosè & longè, Polonè (elektwo & Komèsyal) Recuit & marinated koube, machinn elatriye. |
| Espesyalize nan | Gwo Dyamèt Inconel 625 tiyo |
| Inconel 625 tiyo dimansyon ANSI/ ASME B36.10, B36.19, B2.1 | |
Inconel625 / UNS N06625 /2.4856 Konpozisyon chimik
2.4856 Inconel 625Dimansyon Tablo Tiyo Orè 40
| Gwosè nominal [pous] | Dyamèt deyò [pous] | Dyamèt deyò [mm] | Epesè miray [pous] | Epesè miray [mm] | Pwa [lb/ft] | Pwa [kg/m] |
| 1/8 | 0.405 | 10.3 | 0.068 | 1.73 | 0.24 | 0.37 |
| 1/4 | 0.54 | 13.7 | 0.088 | 2.24 | 0.42 | 0.84 |
| 1/2 | 0.84 | 21.3 | 0.109 | 2.77 | 0.85 | 1.27 |
| 3/4 | 1.05 | 26.7 | 0.113 | 2.87 | 1.13 | 1.69 |
| 1 | 1.315 | 33.4 | 0.133 | 3.38 | 1.68 | 2.5 |
| 1.25 | 1.66 | 42.2 | 0.14 | 3.56 | 2.27 | 3.39 |
| 1.5 | 1.9 | 48.3 | 0.145 | 3.68 | 2.72 | 4.05 |
| 2 | 2.375 | 60.3 | 0.154 | 3.91 | 3.65 | 5.44 |
| 2.5 | 2.875 | 73 | 0.203 | 5.16 | 5.79 | 8.63 |
| 3 | 3.500 | 88.9 | 0.216 | 5.49 | 7.58 | 11.29 |
| 3.5 | 4.000 | 101.6 | 0.226 | 5.74 | 9.11 | 13.57 |
| 4 | 4.500 | 114.3 | 0.237 | 6.02 | 10.79 | 16.07 |
| 5 | 5.563 | 141.3 | 0.258 | 6.55 | 14.62 | 21.77 |
| 6 | 6.625 | 168.3 | 0.28 | 7.11 | 18.97 | 28.26 |
| 8 | 8.625 | 219.1 | 0.322 | 8.18 | 28.55 | 42.55 |
| 10 | 10.75 | 273 | 0.365 | 9.27 | 40.48 | 60.31 |
| 12 | 12.75 | 323.8 | 0.406 | 10.31 | 53.52 | 79.73 |
| 14 | 14 | 355.6 | 0.375 | 11.13 | 54.57 | 94.55 |
| 16 | 16 | 406.4 | 0.5 | 12.7 | 82.77 | 123.3 |
| 18 | 18 | 457 | 0.562 | 14.27 | 104.67 | 155.8 |
| 20 | 20 | 508 | 0.594 | 15.09 | 123.11 | 183.42 |
| 24 | 24 | 610 | 0.688 | 17.48 | 171.29 | 255.41 |
| 32 | 32 | 813 | 0.688 | 17.48 | 230.08 | 342.91 |
ASME SB444 UNS N06625 Aplikasyon pou tiyo san pwoblèm:
- Endistri lwil oliv ak gaz
- Sistèm tiyo, tiyo ak zouti pou twou
- Plant pwosesis chimik
- Echanjeur chalè, veso reyaksyon
- Endistri Aerospace, pou konpozan motè turbine gaz ak sistèm tiyo echapman.
FAQ
K: Konsènan Inconel 625 pri tiyo san pwoblèm pou chak kg?
K: Konbyen tan tan livrezon ou pran?
K: Èske gen sèvis echantiyon?
K: Ki kantite minimòm lòd?
K: Ki jan yo pake pwodwi yo?
K: Peyi ekspòte yo
Baj popilè: inconel 625 tiyo san pwoblèm, astm b444 inconel 625, uns n06625, astm b444