Alloy N06625 Tib
1. Creole: ASTM B444, ASME SB444, ASTM B474, ASME SB474
2. dyamèt: 5. 0 mm - 1219.2 mm
3. epesè miray: 0. 5 - 20 mm
4. Longè: Single o aza, doub o aza & koupe longè.
ASTM B444 UNS N06625 (Inconel 625)se yon alyaj gwo tanperati ki baze sou nikèl. Akòz ekselan rezistans korozyon li yo, gwo fòs ak ekselan estabilite segondè-tanperati, li okipe yon pozisyon enpòtan nan-wo fen jaden endistriyèl tankou avyon, jeni marin, petrochemicals ak enèji nikleyè. HT tiyo se yon inconel 625 founisè tiyo ak 15+ ekspòtasyon eksperyans.Kontakte nouPou plis enfòmasyon ak quotes pou gratis!
Konpozisyon chimik nan Inconel 625
Konpozisyon chimik alyaj 625 la se sitou nikèl (Ni) (kontablite pou apeprè 58%-63%), epi li se optimize pèfòmans reyalize pa ajoute eleman kle tankou CHROMIUM (Cr, 20%-23%), Molibdenum (Mo, 8%-10}, ak Ni (N (2%-10. 3.15%-4. 15%).
Pwopriyete fizik ak mekanik alyaj 625
Tipik fòs la rupture nan alyaj 625 tib nan tanperati chanm ka rive jwenn plis pase 830 MPa, fòs la sede depase 410 MPa, ak elongasyon a se sou 30%, ki montre ekselan plastisit ak severite. Dansite li se sou 8.44 g/cm³, ak pwen k ap fonn li yo se ant 1290-1350 degre. Nan anviwònman tanperati ki wo (tankou anba a 650 degre), alyaj la ka toujou kenbe segondè fluaj rezistans.
Tès materyèl nan inconel 625 tiyo
- Tès dite
- Analiz chimik - analiz spectro
- Idantifikasyon materyèl pozitif - tès PMI
- Tès plat
- Mikwo ak macrotest
- Pitting tès rezistans
- Flaring Tès
- Tès kowozyon intergranular (IGC)

Alloy 625 espesifikasyon tiyo
| Estanda ak klas | ASTM B444 UNS N06625 |
| 625 kalite materyèl | Alyaj nikèl-chromium-molibden-kolonbi |
| Estanda | ASTM, ASME, JIS, AISI, AMS, EN, SAE, DIN, NF, TOCT, DS, DTD, GB |
| Kalite Faktori | San pwoblèm cho woule, rkwit; Soude |
| Gwosè | 1/2 "a 16" |
| Epesè miray | Sch10, Sch 20, Sch 40, Sch Std, Sch 80, Sch Xs, Sch 160 |
| Longè | 6 mèt, 12 mèt, oswa Customized. |
Kowozyon rezistans nan inconel N06625 tiyo
In oxidizing media (such as nitric acid and concentrated sulfuric acid), the passivation effect of chromium makes its corrosion resistance better than most stainless steels, in reducing environments (such as hydrochloric acid and phosphoric acid), the combination of molybdenum and nickel effectively resists local corrosion (such as pitting and crevice corrosion).
Pèfòmans tanperati ki wo nan Inconel 2.4865 tiyo
Nan jaden an tanperati ki wo, Inconel 625 tiyo ka kenbe estabilite estriktirèl pou yon tan long anba a 980 degre. Fòs tanperati ki wo li yo sitou soti nan solisyon solid ranfòse efè nan molibden ak niobium, ak ranfòse a presipitasyon nan faz '' (Ni₃nb).
Pwosesis fabrikasyon nan Inconel N06625 Tib
Manifakti a nan tiyo alyaj 625 enplike nan teknoloji egzak cho ak frèt pwosesis. Se èkstruzyon cho oswa cho pwosesis woule anjeneral te pote soti nan 1150-1200 degre, ki te swiv pa tretman solisyon (dlo quenching nan sou 1100 degre) elimine estrès pwosesis ak optimize estrikti grenn jaden. Deformation a ta dwe kontwole pandan pwosesis frèt pou fè pou evite redi twòp, ak entèmedyè rkwir ka retabli plastisit la nan materyèl la.
soude nan alyaj N06625 tiyo
Alloy 625 la ka soude pa TIG, MIG oswa soude lazè, men matche ERNICRMO -3 fil soude yo ta dwe chwazi, ak tanperati a entèraksyon yo ta dwe entèdi kontwole (rekòmande yo dwe anba a 150 degre) yo anpeche grenn jaden nan zòn nan chofe-ki afekte yo.
Aplikasyon nan tiyo alyaj 625
Marin Jeni:High-presyon tuyaux, tiyo subsea ak koki presyon soumaren pou dlo lanmè desalination sistèm yo.
Ekipman chimik:Fabrikasyon nan aparèy rejenerasyon asid silfirik ak tuyaux evaporator pou endistri a chlor-alkali.
Aerospace:Kòm tiyo gaz ak eleman sistèm echapman pou motè avyon.
Jaden enèji nikleyè:Itilize nan tuyaux awozaj ak depanse ekipman pwosesis gaz pou réacteurs nikleyè.
Inconel 625 UNS N06625 tiyo kare Rating presyon
| Tay | Egalize | Maksimòm presyon entèn yo, KSI | ||||||
| mm | ||||||||
| 100 degre f | 200 degre f | 300 degre f | 400 degre f | 500 degre f | 600 degre f | 700 degre f | ||
| 1.59 x 0.36 | N06625 | 19.21 | 19.21 | 19.02 | 18.83 | 18.54 | 18.15 | 17.77 |
| 3 x 0.5 | N06625 | 940 | 940 | 930 | 921 | 907 | 888 | 869 |
| 6 x1 | N06625 | 940 | 940 | 930 | 921 | 907 | 888 | 869 |
| 8x1 | N06625 | 681 | 681 | 675 | 668 | 658 | 644 | 630 |
| 8x2 | N06625 | 1476 | 1476 | 1462 | 1447 | 1425 | 1395 | 1366 |
| 10x1 | N06625 | 534 | 534 | 529 | 524 | 516 | 505 | 494 |
| 12x1 | N06625 | 440 | 440 | 435 | 431 | 424 | 415 | 407 |
| 16x1 | N06625 | 324 | 324 | 321 | 318 | 313 | 307 | 300 |
Nikèl alyaj 625 tiyo gwosè
| Nan. | Sch | ASTM B444 Inconel 625 Pipe OD | Kg/m | Tiyo wt |
| mm | mm | |||
| 1/4 | 10S | 13.72 | 0.5 | 1.65 |
| 1/4 | 40S | 13.72 | 0.64 | 2.24 |
| 1/4 | 80S | 13.72 | 0.81 | 3.02 |
| 3/8 | 10S | 17.15 | 0.64 | 1.65 |
| 3/8 | 40S | 17.15 | 0.86 | 2.31 |
| 3/8 | 80S | 17.15 | 1.12 | 3.2 |
| 1/2 | 10S | 21.34 | 1.02 | 2.11 |
| 1/2 | 40S | 21.34 | 1.29 | 2.77 |
| 1/2 | 80S | 21.34 | 1.65 | 3.73 |
| 3/4 | 10S | 26.67 | 1.3 | 2.11 |
| 3/4 | 40S | 26.67 | 1.71 | 2.87 |
| 3/4 | 80S | 26.67 | 2.23 | 3.91 |
| 1 | 10S | 33.4 | 2.13 | 2.77 |
| 1 | 40S | 33.4 | 2.54 | 3.38 |
| 1 | 80S | 33.4 | 3.29 | 4.55 |
| 1 | 160 | 33.4 | 4.3 | 6.352) |
| 1¼ | 10S | 42.16 | 2.73 | 2.77 |
| 1¼ | 40S | 42.16 | 3.44 | 3.56 |
| 1¼ | 80S | 42.16 | 4.53 | 4.85 |
| 1¼ | 160 | 42.16 | 5.69 | 6.352) |
| 1½ | 10S | 48.26 | 3.16 | 2.77 |
| 1½ | 40S | 48.26 | 4.11 | 3.68 |
| 1½ | 80S | 48.26 | 5.49 | 5.08 |
| 2 | 10S | 60.33 | 3.99 | 2.77 |
| 2 | 40S | 60.33 | 5.52 | 3.91 |
| 2 | 80S | 60.33 | 7.6 | 5.54 |
| 2 | 160 | 60.33 | 11.29 | 8.742) |
| 2½ | 10S | 73.03 | 5.35 | 3.05 |
| 2½ | 40S | 73.03 | 8.77 | 5.16 |
| 2½ | 80S | 73.03 | 11.59 | 7.01 |
| 3 | 10S | 88.9 | 6.56 | 3.05 |
| 3 | 40S | 88.9 | 11.47 | 5.49 |
| 3 | 80S | 88.9 | 15.51 | 7.62 |
| 3 | 160 | 88.9 | 21.67 | 11.132) |
| 3½ | 10S | 101.6 | 7.53 | 3.05 |
| 3½ | 40S | 101.6 | 13.78 | 5.74 |
| 3½ | 80S | 101.6 | 18.92 | 8.08 |
| 4 | 10S | 114.3 | 8.5 | 3.05 |
| 4 | 40S | 114.3 | 16.32 | 6.02 |
| 4 | 80S | 114.3 | 22.67 | 8.56 |
| 4 | 160 | 114.3 | 34.05 | 13.492) |
| 5 | 40S | 141.3 | 22.1 | 6.55 |
| 5 | 80S | 141.3 | 31.44 | 9.53 |
| 5 | 160 | 141.3 | 49.87 | 15.882) |
| 6 | 10S | 168.28 | 14.04 | 3.4 |
| 6 | 40S | 168.28 | 28.69 | 7.11 |
| 6 | 80S | 168.28 | 43.21 | 10.97 |
| 6 | 120 | 168.28 | 54.75 | 14.27 |
| 6 | 160 | 168.28 | 68.59 | 18.262) |
| 8 | 40S | 219.08 | 43.2 | 8.18 |
| 8 | 80S | 219.08 | 65.63 | 12.7 |
| 8 | 120 | 219.08 | 91.3 | 18.23 |
| 8 | 160 | 219.08 | 112.97 | 23.012) |
FAQ
K: sou pri alyaj 625 tiyo?
A: Pri soti nan chenn $ 30 - $ 35 pou chak kilogram, varye depann sou gwosè, epesè miray, founisè elatriye.
K: Konbyen tan tan livrezon ou pran?
A: Tan livrezon se nan 5-21 jou
K: Èske gen echantiyon sèvis?
A: echantiyon yo bay gratis nan
K: Ki kantite lòd minimòm lan?
A: Pa gen kantite lòd minimòm
K: Ki jan yo pake pwodwi yo?
A: kouch enteryè a gen yon papye ki enpèmeyab kouch ekstèn epi li se fiks ak yon palèt an bwa fumigasyon.
K: peyi ekspòte yo
A: Brezil, Lafrik di sid, Endonezi, peyi Zend, Singapore, Malezi, Iran, Larisi, UAE, Chili, Laos, elatriye
K: Èske nou ka vizite faktori ou a?
A: Natirèlman, ou toujou akeyi!
Baj popilè: Alloy N06625 Tib, Inconel N06625 Tib Konpayi fabrikasyon, Inconel 625 Swèd, Alloy 625 Pri ce
Ou ka renmen tou
Voye rechèch