Alloy 825 tiyo

Alloy 825 tiyo


1. estanda: ASTM B423, ASTM B407, ASTM B163
2. Dyamèt: 4.0 - 1219.2 mm
3. Epesè mi: 0.5 a 20mm
4. Longè: Single, Double Random & Koupe Longè
5. Klas: Incoloy 825, UNS N08825, WNR.2.4858
Voye rechèch
Pwodwi Entwodiksyon

Tiyo alyaj 825se yon alyaj nikèl-fè-chromium ak kwiv, molybdène ak Titàn te ajoute. Li gen ekselan rezistans korozyon nan anviwònman tankou oksidasyon ak diminye kondisyon yo. Alloy 2.4858 se patikilyèman rezistan nan asid silfirik ak asid fosfò. Incoloy 825 tou gen rezistans ekselan nan pitting, korozyon fant ak korozyon intergranular ki te koze pa divès kalite pwodwi chimik yo. Tiyo Incoloy 825 gen bon pwopriyete mekanik nan tanperati ki ba ak mwayen wo (540 degre).

 

Incoloy Alloy 825 ASTM Standard:

 

  • Espesifikasyon estanda ASTM B423 pou alyaj nikèl-fè-kwòm-molibdèn-kwiv (UNS N08825, N08221, ak N06845) tiyo san pwoblèm ak tib

 

  • ASTM B407 Standard Spesifikasyon pou nikèl-fè-kwòm alyaj san pwoblèm tiyo ak tib

 

  • ASTM B163 Standard Spesifikasyon pou nikèl san pwoblèm ak nikèl alyaj kondansateur ak chalè-chanjeur tib
Alloy 825 Pipe

ASTM B423 UNS N08825Konpozisyon chimik

Klas Kr Fe Ni C Mn Taks Si S
Inconel 825 19.5 – 23.5 1.0 max 38.0 – 46.0 0.05 max 1.0 max 1.5 – 3.0 0.5 max 0.03 max

 

Alloy 825 tiyo Pwopriyete mekanik

Dansite Pwen k ap fonn Fòs rupture Fòs Sede (0.2% Offset) Elongasyon
8.47 g/cm3 1413 degre (2580 degre F) Psi – 95,000, MPa – 655 Psi – 45,000 , MPa – 310 40%

 

Incoloy 825 tiyo san pwoblèm klas ekivalan

STANDARD WERKSTOFF NR. DEZOLE AFNOR JWENTI ANNWI BS EN OSWA
Inconel / Incoloy 2.4858 N08825 NC 21 Fedu XH38bt NCF 825 NA 16 NiCr21Mo ЭП703

 

Kontakte kounye a

Incoloy 825 soude tiyo epesè ak dimansyon

GWO NOMINAL [PUS] DYAMET DEYÒ (OD) [PUS] DYAMET DEYÒ (OD) [MM] Epesè MI [POU] Epesè mi [MM] PWA [LB/FT] PWA [KG/M]
1/8" NPS 6 0.41 10.3 0.068 1.73 0.24 0.37
1/4" NPS 8 0.54 13.7 0.088 2.24 0.42 0.63
3/8" NPS 10 0.68 17.1 0.091 2.31 0.57 0.84
1/2" NPS 15 0.84 21.3 0.109 2.77 0.85 1.27
3/4" NPS 20 1.05 26.7 0.113 2.87 1.13 1.69
1" NPS 25 1.32 33.4 0.133 3.38 1.68 2.5
1 1/4" NPS 32 1.66 42.2 0.14 3.56 2.27 3.39
1 1/2" NPS 40 1.9 48.3 0.145 3.68 2.72 4.05
2" NPS 50 2.375 60.3 0.154 3.91 3.65 5.44
2 1/2" NPS 65 2.875 73 0.203 5.16 5.79 8.63
3" NPS 80 3.5 88.9 0.216 5.49 7.58 11.29
3 1/2" NPS 90 4 101.6 0.226 5.74 9.11 13.57
4" NPS 100 4.5 114.3 0.237 6.02 10.79 16.07
5" NPS 125 5.563 141.3 0.258 6.55 14.62 21.77
6" NPS 150 6.625 168.3 0.28 7.11 18.97 28.26
8" NPS 200 8.625 219.1 0.322 8.18 28.55 42.55
10" NPS 250 10.75 273 0.365 9.27 40.48 60.31
12" NPS 300 12.75 323.8 0.406 10.31 53.52 79.73
14" NPS 350 14 355.6 0.437 11.13 54.57 94.55
16" NPS 400 16 406.4 0.5 12.7 82.77 123.3
18" NPS 450 18 457 0.562 14.27 104.67 155.8
20" NPS 500 20 508 0.594 15.09 123.11 183.42
24" NPS 600 24 610 0.688 17.48 171.29 255.41
32" NPS 800 32 813 0.688 17.48 230.08 342.91

 

ASME SB163 N08825 Tib Fabrication

Founisè tiyo Incoloy 825 ofri yon varyete gwosè ak epesè. Li ka pwodwi lè l sèvi avèk yon varyete teknik fabrikasyon tankou woule cho, desen frèt ak woule frèt. Pwosesis rkwit la se tou yon etap enpòtan nan fabrikasyon tiyo Incoloy alyaj 825 pou asire inifòmite pwopriyete materyèl yo epi elimine nenpòt estrès rezidyèl ki ka lakòz fant oswa echèk.

 

Alloy 825 Pwopriyete soude tib

Tib Alloy 825 tou gen bon soude ak pwopriyete pwosesis, epi li ka fasilman rantre nan lòt pati lè l sèvi avèk divès kalite teknik soude tankou gaz tengstèn arc soude, gaz metal arc soude, ak kouvwi metal arc soude.

 

Aplikasyon pou tiyo ASTM B163 UNS N08825:

  • Pwosesis chimik
  • Petwòl ak gaz natirèl
  • Desalinasyon
  • Endistri nikleyè
  • Aplikasyon marin
  • Tretman dlo egou

 

FAQ

K: Konsènan pri tib Alloy 825 pou chak kg?

A: Pri yo varye ant $30 ak $45 pou chak kg, varye selon gwosè, epesè miray, founisè elatriye.

K: Konbyen tan tan livrezon ou pran?

A: Tan livrezon se nan 5-21 jou

K: Èske gen sèvis echantiyon?

A: Yo bay echantiyon yo gratis

K: Ki kantite minimòm lòd?

A: Pa gen Kantite Lòd Minimòm

K: Ki jan yo pake pwodwi yo?

A: Kouch enteryè a gen yon kouch ekstèn papye ki enpèmeyab epi li fiks ak yon palèt an bwa fumigasyon.

K: Peyi ekspòte yo

A: Brezil, Lafrik di sid, Endonezi, peyi Zend, Singapore, Malezi, Iran, Larisi, UAE, Chili, Laos, elatriye

 

 

Baj popilè: alyaj 825 tiyo, alyaj 825, 825 tiyo, tiyo alyaj, n08825

Voye rechèch

whatsapp

Telefòn

Mel

Rechèch