Alyaj 254 plak smo
1. Creole: ASTM A240, ASME SA240
2. epesè: 0.4mm - 50 mm
3. lajè: 1000 - 2000 mm
4. Longè: 2000mm - 6000 mm
UNS S31254, ke yo rele touAlloy 254 SMO oswa EN 1.4547se yon prim super-Austenitic asye pur ki fèt pou anviwònman yo ki pi agresif korozivite . li gen nivo trè wo nan CHROMIUM (19 . 5-20.5%), nikèl (17.5-18.5%), molybdenum (6.0-7.0%) ak NITOG (MOLYBDEN (6.0-7.0%) ak NITOG. HT tiyo se yonSs 254smo plakFounisè ak 15+ Eksperyans ekspòtasyon .Kontakte nouPou plis enfòmasyon ak quotes pou gratis!
ASTM A240 S31254 Espesifikasyon Plak
| Spesifikasyon | ASTM A240 UNS S31254, ASME SA240, MSRR, AMS, BS |
|---|---|
| Gwosè (mm) | 1000 x 2000, 1220 x 2440, 1500 x 3000, 2000 x 2000, 2000 x 4000 |
| Epesè | 0.1 a 100 mm THK |
| Lajè | 10-2500 mm |
| Longè | 2m, 2.44m, 3m, oswa jan sa nesesè |
| Kaba | HR, CR, 2B, 2D, BA, NON (8), SATIN |
| Rez nan | Mou, difisil, mwatye difisil, trimès difisil, sezon prentan difisil elatriye . |
| Stock nan fòm nan | cho-woule, anwoulman, woulo, sèk, plat, fèy, frèt-woule, teren, korektè, taye lenn, plat, woule, shim, rekouvè |
254 SMO Steel Plak Pwopriyete mekanik
| Densite | Pwen k ap fonn | Fòs rupture | Sede fòs (0.2%konpanse) | Elongasyon |
| 8.0 g/cm3 | 1320-1390 degre | 650 | 300 | 35 % |
Avantaj nan 254smo plak
ss254smo eksepsyonèl rezistans korozyon
Segondè Cr -Mo -N alyaj la bay S31254 rezistans eksepsyonèl nan pitting, twou korozyon, estrès korozyon fann, fatig korozyon ak jeneral korozyon . nan klori oswa anviwònman bromid, S31254 kenbe entegrite kote 316L/304 echwe {5 { byen .
Smo254 segondè fòs mekanik
S31254 gen apeprè de fwa fòs la sede nan 316/304 Nerjaveèi . Sa a pèmèt seksyon mens oswa pi wo evalyasyon presyon nan ekipman . fòs rupture li yo (~ 690-850 MPa nan fèy/bobin, mwens pase oswa egal a 220 Hb) vle di nan tan, li vle di. (elongasyon pi gran pase oswa egal a 35%) asire severite nan sèvis ak fasilite nan fòme .
6mo pèfòmans tanperati ki wo
S31254 se ki estab nan tanperati ki wo . solisyon-nan pi wo a ~ 1150 degre, li konsève fòs ak reziste dekale jiska ~ 600-650 degre nan lè, byen lwen pi bon pase 904L (ki netwaye pi wo a ~ 400 degre) . ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ ~ Konduktivite se relativman wo (~ 14 W/m · K), ki ede nan chalè-Exchanger devwa .
S31254 cho ak frèt woule fèy papye ak sekirite
S31254 ofri bon formability ak trè bon weldability . li soude san yo pa pre-chofaj, menm si li travay-hardens byen vit-se konsa filler apwopriye (aws a5 . 14 ernicrmo -3) ak teknik yo ka rekòmande {8} Li kenbe duktilite menm nan tanperati kriyojenik.
Aplikasyon nan fèy SS254SMO
Lwil ak gaz:Tiyo soumaren, zouti downhole pou pwi gaz asid .
Ekipman chimik:Reyaktè asid silfirik, evaporators asid fosfò, ekipman marinated .
Endistri nikleyè:kontenè ak tuyaux pou sistèm tretman dechè nikleyè .
Marin Jeni:Aparèy desalination dlo lanmè, echanjeur chalè .
Pwoteksyon anviwònman:Eleman kle nan fwit gaz gaz desulfurizasyon (FGD) sistèm .

Imperial Dimansyon & gwosè 254 plak SMO nan stock
| Alyaj 254 sifas plak smo fini | Epesè (nan) | Lajè (nan) |
| Ba mexinox sèlman | 18–28 | max . 48 |
| 1 - cho woule, chalè trete, marinated a240 uns s 31254 254 plak alyaj smo & fèy papye | .1000 – .3750 | max . 72 |
| 2R-frèt-woule, klere-ralanti 254 plak SMO | 0.002–0.06 | 0.118–25.551 |
| 2H - travay fè tèt di toujou klas 1.4547 254 smo aisi plak & fèy | 0.002–0.06 | 0.118–24.803 |
| 2b - frèt woule, chalè trete, marinated, po pase 254 SMO Super duplex fèy & plak | 10–24 | max . 72* |
| 2d - frèt woule, chalè trete, marinated 254 plak smo | 12–24 | max . 60 |
| Deco woule-sou Mexinox sèlman | 14–28 | max . 48 |
| Avesta 254 SMO Poli Plak & Fèy (pa fwote) | 11–24 | max . 60 |
| Tanperaman woule Mexinox sèlman | 13–29 | max . 48 |
Smo 254 plak pwa
| Epesè | Plak pwa pou chak zòn inite | Densite |
| 3/16 pous | 0.06000 liv/nan ²42.184176 kg/m² | 0.315 liv/in ³8.72 g/cm³ |
| 1/4 pous | 0.08 liv/nan ²56.245568 kg/m² | 0.315 liv/in ³8.72 g/cm³ |
| 3/8 pous | 0.121 liv/nan ²85.0714216 kg/m² | 0.315 liv/in ³8.72 g/cm³ |
| 1/2 pous | 0.161 liv/nan ²113.1942056 kg/m² | 0.315 liv/in ³8.72 g/cm³ |
| 5/8 pous | 0.196 liv/nan ²137.8016416 kg/m² | 0.315 liv/in ³8.72 g/cm³ |
| 3/4 pous | 0.235 liv/nan ²165.221356 kg/m² | 0.315 liv/in ³8.72 g/cm³ |
| 7/8 pous | 0.274 liv/nan ²192.6410704 kg/m² | 0.315 liv/in ³8.72 g/cm³ |
| 1 pous | 0.313 liv/nan ²220.0607848 kg/m² | 0.315 liv/in ³8.72 g/cm³ |
| 1 1/4 pous | 0.391 liv/nan ²274.9002136 kg/m² | 0.315 liv/in ³8.72 g/cm³ |
| 1 1/2 pous | 0.47 liv/nan ²330.442712 kg/m² | 0.315 liv/in ³8.72 g/cm³ |
| 1 3/4 pous | 0.549 liv/nan ²385.9852104 kg/m² | 0.315 liv/in ³8.72 g/cm³ |
| 2 pous | 0.627 liv/nan ²440.8246392 kg/m² | 0.315 liv/in ³8.72 g/cm³ |
| 2 1/4 pous | 0.705 liv/nan ²495.664068 kg/m² | 0.315 liv/in ³8.72 g/cm³ |
| 2 1/2 pous | 0.784 liv/nan ²551.2065664 kg/m² | 0.315 liv/in ³8.72 g/cm³ |
| 2 3/4 pous | 0.862 liv/nan ²606.0459952 kg/m² | 0.315 liv/in ³8.72 g/cm³ |
| 3 pous | 0.941 liv/nan ²661.5884936 kg/m² | 0.315 liv/in ³8.72 g/cm³ |
FAQ
K: sou pri plak 254SMO?
A: Pri soti nan chenn $ 5 - $ 15 pou chak kilogram, varye depann sou gwosè, epesè miray, founisè elatriye .
K: Konbyen tan tan livrezon ou pran?
A: Tan livrezon se nan 5-21 jou
K: Èske gen echantiyon sèvis?
A: echantiyon yo bay gratis nan
K: Ki kantite lòd minimòm lan?
A: Pa gen kantite lòd minimòm
K: Ki jan yo pake pwodwi yo?
A: kouch enteryè a gen yon papye ki enpèmeyab kouch ekstèn epi li se fiks ak yon fumigasyon an bwa palèt .
K: peyi ekspòte yo
A: Brezil, Lafrik di sid, Endonezi, peyi Zend, Singapore, Malezi, Iran, Larisi, UAE, Chili, Laos, elatriye
K: Èske nou ka vizite faktori ou a?
A: Natirèlman, ou toujou akeyi!
Baj popilè: alyaj 254 plak smo, ss254smo plak manifaktirè, s31254 pri plak, Smo254 founisè
Pwochen
2205 tiyo duplexOu ka renmen tou
Voye rechèch